Fracture mechanism of a coarse-grained magnesium alloy during fracture toughness testing
- 23 January 2009
- journal article
- research article
- Published by Taylor & Francis in Philosophical Magazine Letters
- Vol. 89 (1) , 2-10
Abstract
The fracture mechanism during fracture toughness testing has been investigated on a coarse-grained magnesium alloy, with an average grain size of ∼50 µm, and a low fracture toughness. The results show that {1012}-type deformation twins are formed at the crack tip and many dislocations pile up on these boundaries. The accumulated strains at these boundaries become the origin of fracture; i.e. cracks propagate along these boundaries between the deformation twins and the matrix.Keywords
This publication has 25 references indexed in Scilit:
- Fracture toughness in direct extruded Mg–Al–Zn alloysJournal of Materials Research, 2007
- Simulation of deformation twins and deformation texture in an AZ31 Mg alloy under uniaxial compressionActa Materialia, 2007
- Twinning and texture development in two Mg alloys subjected to loading along three different strain pathsActa Materialia, 2007
- High fracture toughness of extruded Mg–Zn–Y alloy by the synergistic effect of grain refinement and dispersion of quasicrystalline phaseScripta Materialia, 2007
- Hardening evolution of AZ31B Mg sheetInternational Journal of Plasticity, 2007
- Twinning-induced softening in polycrystalline AM30 Mg alloy at moderate temperaturesScripta Materialia, 2006
- Deformation and texture evolution in AZ31 magnesium alloy during uniaxial loadingActa Materialia, 2006
- Influence of grain size on the compressive deformation of wrought Mg–3Al–1ZnActa Materialia, 2004
- Fatigue Crack Initiation Behavior in Ultrafine-Grained Steel Observed by AFM and EBSPJSME International Journal Series A, 2004
- Study of slip mechanisms in a magnesium alloy by neutron diffraction and modelingScripta Materialia, 2003