Grain Size in Aluminum Alloy 6061 under Hot Ring Compression Test and after T6 Temper
Open Access
- 8 April 2017
- journal article
- research article
- Published by MDPI AG in Applied Sciences
- Vol. 7 (4) , 372
Abstract
Peripheral coarse grain during and after hot forming is often a major inconvenience for manufacturing aluminum alloy parts. Not only is the strength reduced, but the subsequent surface treatments are also hard to realize. The literature has shown that peripheral coarse grain is very likely induced by the previous process, such as extrusion. To investigate if peripheral coarse grain could be caused solely by hot forming, this study removed the billet surface layers. This eliminates the effect from the previous processes preparing the billets and forms ring specimens for executing ring compression test. The ring compression test can reveal the friction circumstance of the specimen to the die surface and create versatile deformation in the specimens to simulate forging situations, thereby providing multifaceted conditions to develop diverse grain size in specimen, particularly on its surface. The experiments were designed and analyzed under the Taguchi method, with consideration for factors such as working temperature, speed and amount of compression, and lubricant. Under each experiment, no peripheral coarse grains were found in the specimen, which were peeled and compressed, and even the average grain size after compression test is larger than that of the received billet. No peripheral coarse grains were found in the subsequent T6 temper either, which could, however, refine the grains.Keywords
This publication has 5 references indexed in Scilit:
- A novel processing route for the manufacture of EN AW 6082 forged componentsMaterials Research Innovations, 2015
- Cooling slope casting to produce EN AW 6082 forging stock for manufacture of suspension componentsTransactions of Nonferrous Metals Society of China, 2014
- The effect of processing and Mn content on the T5 and T6 properties of AA6082 profilesJournal of Materials Processing Technology, 2006
- On the grain size refinement of TiAl alloys by cyclic heat treatmentMaterials Science and Engineering: A, 2002
- The Validity of Mathematical Solutions for Determining Friction From the Ring Compression TestJournal of Lubrication Technology, 1970