Effect of different surface treatments on the repair bond strength between aged and new alkasite based restorative material
Open Access
- 6 June 2024
- journal article
- research article
- Published by F1000 Research Ltd in F1000Research
- Vol. 13, 319
Abstract
Background This study investigates various surface treatment methods to assess shear bond strength between set Cention N (alkasite-based restorative material) and new alkasite based restorative material. Assessing different surface treatments provide insights in optimizing repair procedure that enables durability of the restoration, thus potentially benefitting clinical outcomes. Methods A total of 48 alkasite based restorative material blocks, measuring 4 mm in depth and 4 mm in diameter, were prepared. The samples were randomly divided into 8 groups (n = 6) according to the surface treatment done. Group I: Surface preparation by bur; Group II: Surface treatment by laser; Group III: Application of 2-step etch and rinse adhesive (Adper Single Bond 2 adhesive),Group IV: Application of single step self-etch adhesive (Scotchbond Universal adhesive); Group V: Bur preparation followed by application of 2-step etch and rinse adhesive; Group VI: Bur preparation followed by application of single step self-etch adhesive; Group VII: Laser preparation followed by application of 2-step etch and rinse adhesive; and Group VIII: Laser preparation followed by application of single step self-etch adhesive. Post-surface preparation, all the specimens were restored with newly mixed alkasite material. Repair bond strength measurements were assessed with universal testing machine. Shapiro-Wilk and Levene's tests were used to check normality and Homogeneity of variance. ANOVA with post-hoc Games-Howell test and two-way ANOVA with post-hoc Bonferroni test was performed to evaluate the influence of surface preparation on the repair bond strength. Results Using a 2-step etch and rinse adhesive resulted in a higher repair bond strength (26.05±2.12) compared to other surface treatments. In contrast, roughening of the surface with burs led to lowest repair bond strength (17.06±3.29) (P=0.02). Conclusion Application of 2-step etch and rinse adhesive to the existing alkasite based restorative material provides superior bonding with the newly added alkasite based restorative material.Keywords
This publication has 22 references indexed in Scilit:
- Repair of aged restorations made in direct resin composite – A systematic reviewInternational Journal of Adhesion and Adhesives, 2023
- Retrospective analysis on the repair vs. replacement of composite restorationsDental Materials, 2020
- Efficacy of different surface treatments and universal adhesives on the microtensile bond strength of bulk-fill composite repairJournal of Adhesion Science and Technology, 2019
- Can repair increase the longevity of composite resins? Results of a 10-year clinical trialJournal of Dentistry, 2015
- Repair of restorations – Criteria for decision making and clinical recommendationsDental Materials, 2013
- Comparison of the Effect of Three Mechanical Surface Treatments on the Repair Bond Strength of a Laboratory CompositePhotomedicine and Laser Surgery, 2010
- Effect of surface conditioning methods on the microtensile bond strength of resin composite to composite after aging conditionsDental Materials, 2007
- Bonding of composite to water aged composite with surface treatmentsDental Materials, 2007
- The effect of various surface treatments and bonding agents on the repaired strength of heat-treated compositesThe Journal of Prosthetic Dentistry, 2001
- Adverse surface interactions between one-bottle light-cured adhesives and chemical-cured compositesDental Materials, 2001