Abstract
This report describes progress made in the first half of Phase II of a three-phase program to develop high-efficiency, same-band-gap, amorphous-silicon, tandem-junction modules. Results for both 1-cm- {sup 2} devices and 0.3-m (0.09-m{sup 2}) modules are given. considerable effort was devoted to finding a device structure and layer conditions that reconcile the conflicting requirements of a good ``tunnel junction`` contact between the two stacks and a high-efficiency device. High-band-gap p{sub 2}layers, which enable good voltage and current from the second stack, were found to result in poor tunnel junctions. The best results were obtained by using a thin (1-nm-thick) p{sup +} layer (no carbon) between the n{sub 1} and p{sub 2} layers of the device.