Abstract
Austenitic stainless steel (AISI) 304 is known to have excellent corrosion resistance under atmospheric conditions. However, corrosion resistance in austenitic stainless steel 304 can decrease in a medium containing chloride ions. In this work, the effects of the concentration of sodium chloride solution on microstructure, crystal phases, elemental composition, and corrosion behavior of AISI 304 were focused on by using a digital light microscope, SEM-EDS, XRD, XRF, and linear sweep voltammetry techniques. Various sodium chloride concentrations were prepared at 1%; 2%; 3.5%; 4%; and 5%. The AISI 304 samples were treated mechanically by polishing on the surface, then comparing it to the unpolished samples. Austenitic and ferrite phases were observed in a cubic structure. Iron (Fe), chromium (Cr), nickel (Ni), manganese (Mn), and carbon (C) were found as the major elements. After the AISI 304 samples were immersed in a chlorinated solution, the corrosion from pitting, intergranular, and rust was observed only on the surfaces of the unpolished samples. However, the changes for the crystal structures and major elemental compositions were insignificant when the concentration of chlorinated solution increased. On the other hand, an increase in the corrosion rate was observed. The lowest corrosion resistance of AISI 304 was found at 5% NaCl. When the NaCl concentration increased, the corrosion rate increased.

This publication has 9 references indexed in Scilit: