Abstract
Cellular materials such as aluminum and polyurethane foams are recognized for their effectiveness in energy absorption. They commonly serve as crushable cores in sacrificial cladding for blast mitigation purposes. This study delves into the effectiveness of autoclaved aerated concrete (AAC), a lightweight, porous material known for its energy-absorbing properties as a crushable core in sacrificial cladding. The experimental set-up features a rigid frame made of steel measuring 1000 × 1000 × 15 mm3 with a central square opening (300 × 300 mm2) holding a 2 mm thick aluminum plate representing the structure. The dynamic response of the aluminum plate is captured using two high-speed cameras arranged in a stereoscopic configuration. Three-dimensional digital image correlation is used to compute the transient deformation fields. Blast loading is achieved by detonating 20 g of C4 explosive set at 250 mm from the plate’s center. The study assesses the mineral foam’s absorption capacity by comparing out-of-plane displacement and mean permanent deformation of the aluminum plate with and without the protective solution. Six foam configurations (A to F) are tested experimentally and numerically, varying in the foam’s free space for expansion relative to its total volume. Results show positive protective effects, with configuration F reducing maximum deflection by at least 30% and configuration C by up to 70%. Foam configuration influences energy dissipation, with an optimal lateral surface-to-volume ratio (ζ) enhancing protective effects, although excessive ζ leads to non-uniform foam crushing. To address the influence of front skin deformability, a non-deformable front skin has been adopted. The latter demonstrates an increased effectiveness of the sacrificial cladding, particularly for ζ values above the optimal value obtained when using a deformable front skin. Notably, using a non-deformable front skin increases maximum deflection reduction and foam energy absorption by up to approximately 30%.Keywords
This publication has 47 references indexed in Scilit:
- Dual-mechanism auxetic-core protective sandwich structure under blast loadingComposite Structures, 2022
- Blast protection of steel reinforced concrete structures using composite foam-core sacrificial claddingComposites Science and Technology, 2022
- Blast mitigation by water mist: the effect of the detonation configurationShock Waves, 2020
- Blast resistance of auxetic and honeycomb sandwich panels: Comparisons and parametric designsComposite Structures, 2018
- Shock Wave Interactions2018
- Estimation of the Strain Rate Hardening of Aluminium Using an Inverse Method and Blast LoadingJournal of Dynamic Behavior of Materials, 2017
- Mitigation of Accelerations Caused by Blast Loading Utilizing Polymeric-Coated Metallic Thin-Walled CylindersJournal of Dynamic Behavior of Materials, 2015
- Blast performance of a sacrificial cladding with composite tubes for protection of civil engineering structuresComposites Part B: Engineering, 2014
- Numerical modeling of large deformations in soil structure interaction problems using FE, EFG, SPH, and MM-ALE formulationsArchive of Applied Mechanics, 2014
- Experimental investigation on the shock-wave load attenuation by geometrical meansShock Waves, 2009