Abstract
Nickel Alloys and Molten Chloride salts are the forefront of research for high temperature materials in power generation and advanced nuclear power systems. There exist Increasing interest in Molten Salt Reactors that use molten salt as a coolant or as a fuel, these reactors have been proven to operate with improved safeguards. Chloride Molten Salt’s properties make it a great heat transfer fluid (HTF) and it is an ideal candidate for Thermal Energy Storage (TES). These applications are faced with the challenges of material corrosion caused by the Molten Chloride Salt. Thermo-mechanical derating is especially relevant for next generation molten salt systems targeting ≥ 700 °C operation [1]. Sensitization is the development of chromium depleted grain boundary regions, often associated with carbide precipitation, that promote intergranular corrosion and cracking; it is commonly quantified using electrochemical reactivation metrics such as the DL‑EPR ratio Ir/Ia to determine the degree of sensitization (DOS), another method is measuring the carbon forming carbide to be greater than 0.008 wt% [2]. We examine how chloride molten salt drive selective element dissolution, notably Cr, porous depleted surface layers, and grain-boundary attack, with strong dependence on temperature, stress strain, exposure time, salt redox state, and oxygen water impurities. The paper’s objective is to establish a mechanistically grounded linkage between salt chemistry, impurity control, sensitization metrics (DoS, intergranular attack depth), and derating factors suitable for design and qualification testing.

This publication has 27 references indexed in Scilit: