Abstract
Fe-7, 8, 9, and 11%Si-Cr powders were gas-atomized and then annealed at 25-750 $^{\rm o}$ C to investigate the effects of Si content, DO $_3$ phase, and B2 phase on the high-frequency permeability of the powders. The formation of the B2 phase could not be suppressed during the atomization process of all the powders. The evolution temperatures of the DO $_3$ phase in the Fe-7, 8, and 9%Si-Cr powders as measured by XRD were 550, 550, and 450 $^{\rm o}$ C, respectively. As the annealing temperature was increased, the DO $_3$ phase grew rapidly, and the lattice parameters of the powders were decreased except for those of the Fe-11%Si-Cr powder. The coercivity of all powders decreased with increasing temperature; however, the coercivity of the Fe-8, 9%Si-Cr powders increased sharply after annealing at 450 $^{\rm o}$ C. Permeability decreased rapidly with increasing temperature except for the Fe-11%Si-Cr powder; thus, the highest real permeability was obtained for the as-atomized Fe-8%Si-Cr powder. The changes in the coercivity and permeability of the powders with annealing temperature could be attributed to the evolution of the DO $_3$ phase, Si segregation, and changes in electrical resistivity.

This publication has 11 references indexed in Scilit: