Pyungwoo Jang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Pyungwoo Jang has a total of 15 co-authors. Here are the top co-authors by number of shared publications:
Gwangbo Choi
Central Research and Development Center, Changsung Corporation, Incheon, South Korea
3 shared publications- Kwang Ho Kim
Department of Materials Science and Engineering, Pusan National University, 2 Busandaehak-ro 63 beon-gil, Geumjeong-gu, Busan 46241, Republic of Korea
2 shared publications Kyu Seomoon
Cheongju University
2 shared publicationsBonghan Lee
Division of Applied Science, Cheongju University, Cheongju 360-764, Korea
1 shared publicationByungcheol Lee
Division of Free Electron Laser, Korea Atomic Energy Institute, Daejeon 305-353, Korea
1 shared publication- Chi Sup Jung
Department of Optical Engineering, Cheongju University, Cheongju, 360-764, South Korea
1 shared publication
Latest Publications
- Open Access
- 5 September 2018
- Published by The Korean Institute of Metals and Materials in Korean Journal of Metals and Materials
- Vol. 56 (9) , 680-685
Effects of Annealing on Structure and Magnetic Properties of Fe-Si-Al Flakes
- 5 September 2018
- Published by The Korean Institute of Metals and Materials in Korean Journal of Metals and Materials
- Vol. 56 (9) , 680-685
Open AccessEffects of Annealing on Structure and Magnetic Properties of Fe-Si-Al Flakes
- 28 February 2018
- Published by The Korean Magnetics Society in Journal of the Korean Magnetics Society
- Vol. 28 (1) , 5-9
Core Loss Measurement of dc-Biased Soft Magnetic Composite Cores
Core losses of dc-biased Fe-Si-Al and Fe-Ni cores were measured. Changes of shapes and amplitude of ac loops, and permeability were attributed from the incremental permeability derived from dc loops. Core loss decreased with increasing dc field and then increased abruptly regardless of frequency in the cores with high permeability. It seemed that the decrease of the core loss with increasing dc field was attributed from decrease of dc hysteresis loss. Increase of the loss was seemed to be attributed from increase of amplitude of ac field which was also due to decrease of incremental permeability.
- 28 February 2018
- Published by The Korean Magnetics Society in Journal of the Korean Magnetics Society
- Vol. 28 (1) , 5-9
Core Loss Measurement of dc-Biased Soft Magnetic Composite Cores
Core losses of dc-biased Fe-Si-Al and Fe-Ni cores were measured. Changes of shapes and amplitude of ac loops, and permeability were attributed from the incremental permeability derived from dc loops. Core loss decreased with increasing dc field and then increased abruptly regardless of frequency in the cores with high permeability. It seemed that the decrease of the core loss with increasing dc field was attributed from decrease of dc hysteresis loss. Increase of the loss was seemed to be attributed from increase of amplitude of ac field which was also due to decrease of incremental permeability.
- 15 May 2017
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Magnetics
- Vol. 53 (11) , 1-5
Effects of Silicon Content on the Properties of Gas-Atomized Fe–Si–Cr Powders
Fe-7, 8, 9, and 11%Si-Cr powders were gas-atomized and then annealed at 25-750 $^{\rm o}$ C to investigate the effects of Si content, DO $_3$ phase, and B2 phase on the high-frequency permeability of the powders. The formation of the B2 phase could not be suppressed during the atomization process of all the powders. The evolution temperatures of the DO $_3$ phase in the Fe-7, 8, and 9%Si-Cr powders as measured by XRD were 550, 550, and 450 $^{\rm o}$ C, respectively. As the annealing temperature was increased, the DO $_3$ phase grew rapidly, and the lattice parameters of the powders were decreased except for those of the Fe-11%Si-Cr powder. The coercivity of all powders decreased with increasing temperature; however, the coercivity of the Fe-8, 9%Si-Cr powders increased sharply after annealing at 450 $^{\rm o}$ C. Permeability decreased rapidly with increasing temperature except for the Fe-11%Si-Cr powder; thus, the highest real permeability was obtained for the as-atomized Fe-8%Si-Cr powder. The changes in the coercivity and permeability of the powders with annealing temperature could be attributed to the evolution of the DO $_3$ phase, Si segregation, and changes in electrical resistivity.- 15 May 2017
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Magnetics
- Vol. 53 (11) , 1-5
Effects of Silicon Content on the Properties of Gas-Atomized Fe–Si–Cr Powders
Fe-7, 8, 9, and 11%Si-Cr powders were gas-atomized and then annealed at 25-750 $^{\rm o}$ C to investigate the effects of Si content, DO $_3$ phase, and B2 phase on the high-frequency permeability of the powders. The formation of the B2 phase could not be suppressed during the atomization process of all the powders. The evolution temperatures of the DO $_3$ phase in the Fe-7, 8, and 9%Si-Cr powders as measured by XRD were 550, 550, and 450 $^{\rm o}$ C, respectively. As the annealing temperature was increased, the DO $_3$ phase grew rapidly, and the lattice parameters of the powders were decreased except for those of the Fe-11%Si-Cr powder. The coercivity of all powders decreased with increasing temperature; however, the coercivity of the Fe-8, 9%Si-Cr powders increased sharply after annealing at 450 $^{\rm o}$ C. Permeability decreased rapidly with increasing temperature except for the Fe-11%Si-Cr powder; thus, the highest real permeability was obtained for the as-atomized Fe-8%Si-Cr powder. The changes in the coercivity and permeability of the powders with annealing temperature could be attributed to the evolution of the DO $_3$ phase, Si segregation, and changes in electrical resistivity.- 26 October 2016
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Magnetics
- Vol. 53 (4) , 1-4
Effects of Ordering on the Magnetic Properties of Gas-Atomized Fe–Si–Cr Powders
Fe-9%Si-2%Cr powder were gas-atomized and then annealed in order to investigate effects of DO3 and B2 ordered phases on high frequency permeability of the powder. The B2 phase formed during the atomization process. The DO3 phase began to form at 450oC and grew rapidly when annealed at higher temperature as confirmed by XRD whereas the existence of the DO3 phase in the asatomized powder could be confirmed by TEM. With increasing the temperature the average lattice parameter and the coercivity decreased. There was an abrupt increment of the coercivity in the powder annealed at 450oC. Highest permeability could be obtained in the powder annealed at a relative low temperature of 150oC and then the permeability real decreased with the temperature. The behavior of the coercivity and the permeability with the temperature could be successfully explained by the formation of the DO3 ordered phase and the change of the electrical resistivity.
- 26 October 2016
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Magnetics
- Vol. 53 (4) , 1-4
Effects of Ordering on the Magnetic Properties of Gas-Atomized Fe–Si–Cr Powders
Fe-9%Si-2%Cr powder were gas-atomized and then annealed in order to investigate effects of DO3 and B2 ordered phases on high frequency permeability of the powder. The B2 phase formed during the atomization process. The DO3 phase began to form at 450oC and grew rapidly when annealed at higher temperature as confirmed by XRD whereas the existence of the DO3 phase in the asatomized powder could be confirmed by TEM. With increasing the temperature the average lattice parameter and the coercivity decreased. There was an abrupt increment of the coercivity in the powder annealed at 450oC. Highest permeability could be obtained in the powder annealed at a relative low temperature of 150oC and then the permeability real decreased with the temperature. The behavior of the coercivity and the permeability with the temperature could be successfully explained by the formation of the DO3 ordered phase and the change of the electrical resistivity.
- 10 September 2013
- Published by Springer Nature in Metals and Materials International
- Vol. 19 (5) , 1163-1166
Formation of particulate Fe-Al films by selective oxidation of aluminum
- 10 September 2013
- Published by Springer Nature in Metals and Materials International
- Vol. 19 (5) , 1163-1166
Formation of particulate Fe-Al films by selective oxidation of aluminum
- Open Access
- 2 April 2013
- Published by Springer Nature in Discover Nano
- Vol. 8 (1) , 152
Fabrication of Fe-Al nanoparticles by selective oxidation of Fe-Al thin films
The possibility of a new technique for fabricating nanoparticles from thin films using selective oxidation in an atmosphere mixture of water vapor and hydrogen was investigated. Fe-5wt.%Al films were RF-sputtered and annealed in the atmosphere mixture at 900°C for up to 200 min, in order to oxidize aluminum selectively. Thermodynamics simulation showed that temperatures exceeding 800°C are necessary to prevent iron from being oxidized, as confirmed by the depth profile of XPS. As the annealing time increased, the morphology of the 200-nm Fe-Al films changed from the continuous to the discontinuous type; thus, particulate Fe-Al films formed after 100 min. The particulate 10- to 100-nm Fe-Al films showed super-paramagnetic behavior after the oxidation. Thus, a new technique for fabricating nanoparticles was successfully introduced using selective oxidation.
- 2 April 2013
- Published by Springer Nature in Discover Nano
- Vol. 8 (1) , 152
Open AccessFabrication of Fe-Al nanoparticles by selective oxidation of Fe-Al thin films
The possibility of a new technique for fabricating nanoparticles from thin films using selective oxidation in an atmosphere mixture of water vapor and hydrogen was investigated. Fe-5wt.%Al films were RF-sputtered and annealed in the atmosphere mixture at 900°C for up to 200 min, in order to oxidize aluminum selectively. Thermodynamics simulation showed that temperatures exceeding 800°C are necessary to prevent iron from being oxidized, as confirmed by the depth profile of XPS. As the annealing time increased, the morphology of the 200-nm Fe-Al films changed from the continuous to the discontinuous type; thus, particulate Fe-Al films formed after 100 min. The particulate 10- to 100-nm Fe-Al films showed super-paramagnetic behavior after the oxidation. Thus, a new technique for fabricating nanoparticles was successfully introduced using selective oxidation.
- 1 July 2011
- Published by Elsevier in Current Applied Physics
- Vol. 11 (4) , S95-S97
Interfacial structure of ferromagnetic Fe-Pt thin films grown on a Si substrate
- 1 July 2011
- Published by Elsevier in Current Applied Physics
- Vol. 11 (4) , S95-S97
Interfacial structure of ferromagnetic Fe-Pt thin films grown on a Si substrate
- 1 July 2011
- Published by Elsevier in Current Applied Physics
- Vol. 11 (4) , S30-S32
Inductively coupled plasma post-treatment of Al-doped ZnO thin films
- 1 July 2011
- Published by Elsevier in Current Applied Physics
- Vol. 11 (4) , S30-S32
Inductively coupled plasma post-treatment of Al-doped ZnO thin films
- 14 December 2007
- Published by Wiley in Physica Status Solidi (a)
- Vol. 204 (12) , 4194-4197
Feasibility study of micro-undulator for T-ray sources by using FEM
- 14 December 2007
- Published by Wiley in Physica Status Solidi (a)
- Vol. 204 (12) , 4194-4197
Feasibility study of micro-undulator for T-ray sources by using FEM
- 14 December 2007
- Published by Wiley in Physica Status Solidi (a)
- Vol. 204 (12) , 4108-4112
Order‐disorder transition and magnetic properties of Fe‐6.5Si alloy powder cores
Magnetic properties of Fe‐6.5%Si powder compact cores were analyzed when cores were annealed at 400 – 800 °C for up to 960 min. Hysteresis losses were larger than eddy current lossed in all cores. With increasing annealing temperature core loss decreased while eddy current loss showed minimum when annealed at 500 °C. Variation of DC and AC magnetic properties with annealing temperature and time could be successfully explained by order‐disorder transition, magnetostriction, resistivity, lubricant burn‐off, and surface oxidation of particles.
- 14 December 2007
- Published by Wiley in Physica Status Solidi (a)
- Vol. 204 (12) , 4108-4112
Order‐disorder transition and magnetic properties of Fe‐6.5Si alloy powder cores
Magnetic properties of Fe‐6.5%Si powder compact cores were analyzed when cores were annealed at 400 – 800 °C for up to 960 min. Hysteresis losses were larger than eddy current lossed in all cores. With increasing annealing temperature core loss decreased while eddy current loss showed minimum when annealed at 500 °C. Variation of DC and AC magnetic properties with annealing temperature and time could be successfully explained by order‐disorder transition, magnetostriction, resistivity, lubricant burn‐off, and surface oxidation of particles.