Wear Simulation of Ceramic-on-Crosslinked Polyethylene Hip Prostheses: A New Non-Oxide Silicon Nitride versus the Gold Standard Composite Oxide Ceramic Femoral Heads
Authors:
- Makiko YorifujiMYMakiko Yorifuji
- Saverio AffatatoSaverio Affatato
- Toshiyuki TateiwaTTToshiyuki Tateiwa
- Yasuhito TakahashiYTYasuhito Takahashi
- Takaaki ShishidoTSTakaaki Shishido
- Elia MarinElia Marin
- Matteo ZanoccoMZMatteo Zanocco
- Wenliang ZhuWZWenliang Zhu
- Giuseppe PezzottiGPGiuseppe Pezzotti
- Kengo YamamotoKYKengo Yamamoto
Open Access
Abstract
The purpose of the present study was to compare the wear behavior of ceramic-on-vitamin-E-diffused crosslinked polyethylene (Vit-E XLPE) hip bearings employing the gold standard oxide ceramic, zirconia (ZrO2)-toughened alumina (Al2O3) (ZTA, BIOLOX®delta) and a new non-oxide ceramic, silicon nitride (Si3N4, MC2®). In vitro wear test was performed using a 12-station hip joint simulator. The test was carried out by applying the kinematic inputs and outputs as recommended by ISO 14242-1:2012. Vitamin-E-diffused crosslinked polyethylene (Vit-E XLPE) acetabular liners (E1®) were coupled with Ø28-mm ZTA and Si3N4 femoral heads. XLPE liner weight loss over 5 million cycles (Mc) of testing was compared between the two different bearing couples. Surface topography, phase contents, and residual stresses were analyzed by contact profilometer and Raman microspectroscopy. Vit-E XLPE liners coupled with Si3N4 heads produced slightly lower wear rates than identical liners with ZTA heads. The mean wear rates (corrected for fluid absorption) of liners coupled with ZTA and Si3N4 heads were 0.53 ± 0.24 and 0.49 ± 0.23 mg/Mc after 5 Mc of simulated gait, respectively. However, after wear testing, the ZTA heads retained a smoother topography and showed fewer surface stresses than the Si3N4 ones. Note that no statistically significant differences were found in the above comparisons. This study suggests that the tribochemically formed soft silica layer on the Si3N4 heads may have reduced friction and slightly lowered the wear of the Vit-E XLPE liners. Considering also that the toughness of Si3N4 is superior to ZTA, the present wear data represent positive news in the future development of long-lasting hip components.Keywords
This publication has 37 references indexed in Scilit:
- Strain-induced microstructural rearrangement in ultra-high molecular weight polyethylene for hip joints: A comparison between conventional and vitamin E-infused highly-crosslinked linersJournal of the Mechanical Behavior of Biomedical Materials, 2014
- Advances in zirconia toughened alumina biomaterials for total joint replacementJournal of the Mechanical Behavior of Biomedical Materials, 2014
- Vitamin E diffused, highly crosslinked UHMWPE: a reviewInternational Orthopaedics, 2010
- Surface Topology of Advanced Alumina/Zirconia Composite Femoral Head as Compared with Commercial Femoral Heads Made of Monolithic ZirconiaJournal of the American Ceramic Society, 2010
- Raman tensor analysis of ultra-high molecular weight polyethylene and its application to study retrieved hip joint componentsActa Biomaterialia, 2010
- Characterization of protein degradation in serum‐based lubricants during simulation wear testing of metal‐on‐metal hip prosthesesJournal of Biomedical Materials Research Part B: Applied Biomaterials, 2010
- The effects of high dose irradiation on the cross-linking of vitamin E-blended ultrahigh molecular weight polyethyleneBiomaterials, 2008
- Wear Resistance and Mechanical Properties of Highly Cross-linked, Ultrahigh–Molecular Weight Polyethylene Doped With Vitamin EThe Journal of Arthroplasty, 2006
- Advanced nanocomposite materials for orthopaedic applications. I. A long‐term in vitro wear study of zirconia‐toughened aluminaJournal of Biomedical Materials Research Part B: Applied Biomaterials, 2005
- Potential thermal artifacts in hip joint wear simulatorsJournal of Biomedical Materials Research, 1999