Bio‐based poly(trimethylene terephthalate)/polyamide 56 blend fibers via melt spinning: Preparation, structure, and properties
Authors:
- 30 August 2024
- journal article
- research article
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 141 (45)
Abstract
Melt‐spun poly(trimethylene terephthalate) (PTT) and polyamide 56 (PA56) fibers are generally prepared individually. Herein, inspired by the complementary properties of these two materials, PTT/PA56 blend fibers were prepared by two‐step melt spinning and drawing processes. The regularity of crystalline regions, overall orientation in crystalline and amorphous regions, and dimensional stability under hot and humid conditions can be improved by increasing drawing temperature. The most suitable drawing temperature is 90°C, at which 4‐fold drawn PTT and PA56 fibers show tenacity of 2.94 and 3.54 cN/dtex, respectively. An increase in draw ratio leads to increase in the order of crystal regions and overall orientation in crystalline and amorphous phases. Interestingly, increasing dispersed phase content from 0 to 10 wt% is conducive to the increase in tenacity of samples. The PTT/PA56 (10/90) blend fiber suggests the maximum tenacity value, and tenacity of 4‐fold drawn fiber is 4.02 cN/dtex. As PA56 content increases, dimensional stability of samples under dry conditions increases. Comprehensive analysis demonstrates that the PTT/PA56 (10/90) blend fiber achieves the best combination of tensile properties and dimensional stability. The prepared PTT/PA56 blend fibers are potentially competitive in the fields of fibers, garment, and decoration due to their satisfactory comprehensive performances.Keywords
Funding Information
- National Key Research and Development Program of China (2019YFC1904502)
This publication has 47 references indexed in Scilit:
- Structure–property evolution of poly(ethylene terephthalate)/poly(trimethylene terephthalate) side‐by‐side self‐crimp filamentJournal of Applied Polymer Science, 2023
- Structure and properties of bio‐based poly(trimethylene terephthalate)/polyamide 56 blends prepared by melt mixingJournal of Applied Polymer Science, 2023
- Bio‐based polyamide 56 fibers by one‐step melt‐spinning: Process, structure and propertiesJournal of Applied Polymer Science, 2023
- Influence of drawing and annealing on the structure and properties of bio‐based polyamide 56 fibersJournal of Applied Polymer Science, 2022
- Effect of heat treatment with alternating tension on microstructure and elastic recovery of poly(trimethylene terephthalate) fibersPolymers for Advanced Technologies, 2022
- Relationship between the Processing, Structure, and Properties of Microfibrillar CompositesAdvanced Materials, 2020
- The structures and properties of bio‐based polyamide 56 fibers prepared by high‐speed spinningJournal of Applied Polymer Science, 2020
- Recent Advances in 1D Stretchable Electrodes and Devices for Textile and Wearable Electronics: Materials, Fabrications, and ApplicationsAdvanced Materials, 2019
- Blends of polylactide and poly(3‐hydroxybutyrate‐co‐3‐hydroxyvalerate) with low content of hydroxyvalerate unit: Morphology, structure, and propertyJournal of Applied Polymer Science, 2015
- Crystallization, morphology, and electrical properties of bio‐based poly(trimethylene terephthalate)/poly(ether esteramide)/ionomer blendsJournal of Applied Polymer Science, 2010