Long Term Stability of Acrylamide Based Polymers during Chemically Assisted CO2 WAG EOR

Authors:

Abstract
CO2 flooding often results in poor sweep efficiency due to the high mobility ratio caused by its low viscosity. To mitigate this problem, the alternate injection of water and CO2 slugs, known as the water-alternating-gas process (WAG), is widely applied. Recently, numerical simulation and core flood experiments indicate that the use of chemicals in the water slug may improve mobility control during WAG, thus increasing the ultimate recovery and reducing the requirements for newly purchased or recycled CO2. Therefore, the study of the stability of common polymers used for EOR applications in CO2 saturated environments becomes necessary to address the technical and economic feasibility of this process. In this paper, we report the results of two commonly applied EOR polymers, a co-polymer of acrylamide and acrylate and a co-polymer of acrylamide and ATBS (Acrylamide tert-Butyl Sulfonate). To establish a base line for comparison, parallel experiments were conducted in two different oxygen free environments: one with CO2 and the other with nitrogen. Samples were hydrated and aged at reservoir temperature over 300 days. To isolate the effect of CO2, polymer thermal and chemical degradation were reduced by stripping out dissolved oxygen and decreasing divalent cation concentration from the water prior to polymer hydration. Polymer samples were removed at different times and their viscosity was measured as a function of shear rate and fitted to a power law model. The ability of the polymer solutions to retain their original viscosity over time was used to quantify polymer degradation. The results of this work show that CO2 impacts polymer stability, causing further degradation in both polymers tested. The co-polymer of acrylamide and ATBS exhibited higher resistance to CO2 degradation as it was able to retain 94 % of its original viscosity, compared with the co-polymer of acrylamide and acrylate which only retained 56 %. Factors as chemical degradation, hydrolysis and pH, that also affected the behavior of viscosity over time are addressed. We conclude that commercial polymers can be used during chemically assisted CO2 WAG when low divalent cation water is used at a reservoir temperature of 122 F.