Corrosion behavior of precracked SiC f /SiC composites under 1200–1300°C Na 2 SO 4 ‐wet‐oxygen environment
- 16 January 2024
- journal article
- research article
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 107 (6) , 3701-3715
Abstract
SiC f /SiC composites, as promising materials for the hot‐section components of turbine engines, are susceptible to hot corrosion due to the steam environments. Especially, under rotational and thermal stress, numerous microcracks may be generated in the SiC f /SiC ceramic matrix, which can trigger the rapid invasion of corrosive gases and deteriorate the composite mechanical properties. Therefore, it is of great importance to investigate the degradation mechanisms of SiC f /SiC with precracks existing. Here, the corrosion behavior of precracked SiC f /SiC in the Na 2 SO 4 ‐wet‐oxygen environment was evaluated. By comparing mechanical evolution under different corrosion conditions, microfailure mechanisms of SiC f /SiC were revealed. The results indicate that brittle cracking of the matrix and oxidation erosion of fibers are the key factors in reducing the tensile strain of composites. Specifically, the composite damage resistance increases at 67 MPa‐1300°C. At this point, the prestress level is moderate and close to the matrix cracking limit. The prefabricated microcracks can be healed at 1300°C by liquid oxidation products, which hinders cracks bridging large‐scale. This study is conducive to a better understanding of failure mechanisms of SiC f /SiC in complex service environments.Keywords
Funding Information
- National Natural Science Foundation of China (52172111)
- National Key Research and Development Program of China (2022YFB3707700)
This publication has 16 references indexed in Scilit:
- Mechanical behavior of SiC/SiC composites after exposure in high temperature liquid sodium for Sodium Fast Reactors applicationsJournal of Nuclear Materials, 2021
- Microstructure and mechanical performance of SiCf/BN/SiC mini-composites oxidized at elevated temperature from ambient temperature to 1500 °C in airJournal of the European Ceramic Society, 2020
- Effects of cyclic tensile loading on the rupture behavior of orthogonal 3-D woven SiC fiber/SiC matrix composites at elevated temperatures in airJournal of the European Ceramic Society, 2019
- Acoustic emission—A promising and challenging technique for process monitoring in sheet metal formingJournal of Manufacturing Processes, 2017
- High‐Temperature Na 2 SO 4 Deposit‐Assisted Corrosion of Silicon Carbide – I: Temperature and Time DependenceJournal of the American Ceramic Society, 2014
- A clustering method combining differential evolution with the K-means algorithmPattern Recognition Letters, 2011
- Stress-dependent matrix cracking in 2D woven SiC-fiber reinforced melt-infiltrated SiC matrix compositesComposites Science and Technology, 2004
- Stress-rupture of continuous fibre ceramic composites at intermediate temperaturesJournal of Materials Science Letters, 1997
- Molecular diffusion of oxygen and water in crystalline and amorphous silicaPhilosophical Magazine Part B, 1992
- A Cluster Separation MeasureIEEE Transactions on Pattern Analysis and Machine Intelligence, 1979