Hao Qin
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Hao Qin has a total of 34 co-authors. Here are the top co-authors by number of shared publications:
Xiangyu Zhang
4 shared publicationsShaoming Dong
3 shared publicationsYudong Xue
3 shared publicationsBeibei Ma
School of Mechanics and Aerospace Engineering Dalian University of Technology Dalian China
2 shared publicationsChunjing Liao
2 shared publications- Jinshan Yang
State Key Laboratory of High Performance Ceramics and Superfine Microstructure Shanghai Institute of Ceramics Chinese Academy of Sciences Shanghai China
2 shared publications
Latest Publications
- 4 August 2026
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 109 (8) , e71074
Microstructure and Thermophysical Properties of CVD BN Treated at Temperature up to 1550°C
Boron nitride (BN), as an interphase, plays an important role in thermophysical and mechanical properties of continuous fiber‐reinforced ceramic matrix composite. In this work, BN sheets were fabricated by chemical vapor deposition method. To simulate the service temperature, the BN sheets were treated at high temperatures up to 1550°C, and then thermophysical properties at elevated temperatures were investigated. The results exhibited that the high‐temperature treatment promoted the crystallization and structural rearrangement of BN. Particularly, BN treated at 1550°C showed the compacted layer structure. BN treated at 1550°C exhibited the highest thermal conductivities in direction parallel to the deposition direction, with 1.21 W/(m·K) at RT and 1.50 W/(m·K) at 300°C (peak), which were 49.6% and 29.7% higher than those of as‐fabricated BN, respectively. The increase of thermal conductivity was mainly attributed to the improvement of crystallization and the diminishment of defects. Meanwhile, BN treated at 1550°C exhibited the lowest coefficients of thermal expansion in direction perpendicular to the deposition direction, which were 1.13 × 10 −6 /K at 100°C and 1.02 × 10 −6 /K at 900°C, about 29.4% and 26.3% of that as‐fabricated BN. The decrease in coefficient of thermal expansion was primarily dominated by the improvement of texture degree.
- 4 August 2026
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 109 (8) , e71074
Microstructure and Thermophysical Properties of CVD BN Treated at Temperature up to 1550°C
Boron nitride (BN), as an interphase, plays an important role in thermophysical and mechanical properties of continuous fiber‐reinforced ceramic matrix composite. In this work, BN sheets were fabricated by chemical vapor deposition method. To simulate the service temperature, the BN sheets were treated at high temperatures up to 1550°C, and then thermophysical properties at elevated temperatures were investigated. The results exhibited that the high‐temperature treatment promoted the crystallization and structural rearrangement of BN. Particularly, BN treated at 1550°C showed the compacted layer structure. BN treated at 1550°C exhibited the highest thermal conductivities in direction parallel to the deposition direction, with 1.21 W/(m·K) at RT and 1.50 W/(m·K) at 300°C (peak), which were 49.6% and 29.7% higher than those of as‐fabricated BN, respectively. The increase of thermal conductivity was mainly attributed to the improvement of crystallization and the diminishment of defects. Meanwhile, BN treated at 1550°C exhibited the lowest coefficients of thermal expansion in direction perpendicular to the deposition direction, which were 1.13 × 10 −6 /K at 100°C and 1.02 × 10 −6 /K at 900°C, about 29.4% and 26.3% of that as‐fabricated BN. The decrease in coefficient of thermal expansion was primarily dominated by the improvement of texture degree.
- Open Access
- 1 July 2026
- Published by Elsevier in SSRN Electronic Journal
Interfacial shear strength and failure mechanisms of mini-SiCf/SiC composite with Si-doped BN interphase
In the present study, in order to understand the influence of Si-doping in BN interphase on the interfacial shear strength (ISS) of SiC fiber-reinforced SiC composite, the mini SiCf/SiC composite was fabricated by chemical vapor infiltration process, where the 3rd generation SiC fiber coated with Si-doped BN interphase was applied. The content of Si in BN interphase was varied from 0 to 20%. The ISS was evaluated by single fiber push-out test. The interphase morphology, roughness, chemical state, and crystallinity were investigated in detail. It was found that the ISS was affected by the surface morphology, roughness and crystalline structure of the interphase. When the Si content was ≤ 10%, the ISS increased with increasing Si content, which was attributed to the reduced layered structure and the increased surface roughness. At higher Si contents, the crystalline structure of the interphase was seriously disrupted, and the ISS also decreased. The debonding behavior was found to be governed by surface roughness and morphology. Furthermore, the debonding location was observed at the fiber side for composite with a BN interphase, while that changed to the matrix side upon the introduction of Si.
- 1 July 2026
- Published by Elsevier in SSRN Electronic Journal
Open AccessInterfacial shear strength and failure mechanisms of mini-SiCf/SiC composite with Si-doped BN interphase
In the present study, in order to understand the influence of Si-doping in BN interphase on the interfacial shear strength (ISS) of SiC fiber-reinforced SiC composite, the mini SiCf/SiC composite was fabricated by chemical vapor infiltration process, where the 3rd generation SiC fiber coated with Si-doped BN interphase was applied. The content of Si in BN interphase was varied from 0 to 20%. The ISS was evaluated by single fiber push-out test. The interphase morphology, roughness, chemical state, and crystallinity were investigated in detail. It was found that the ISS was affected by the surface morphology, roughness and crystalline structure of the interphase. When the Si content was ≤ 10%, the ISS increased with increasing Si content, which was attributed to the reduced layered structure and the increased surface roughness. At higher Si contents, the crystalline structure of the interphase was seriously disrupted, and the ISS also decreased. The debonding behavior was found to be governed by surface roughness and morphology. Furthermore, the debonding location was observed at the fiber side for composite with a BN interphase, while that changed to the matrix side upon the introduction of Si.
- 7 November 2025
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 109 (1)
A machine learning‐based multi‐scale morphological approach for crack segmentation
To achieve quantitative analysis of cracks in different regions for C f /SiC composites, this study proposes an automated, multi‐scale crack segmentation and quantitative analysis framework for composites with complex backgrounds. This framework is based on the ResNet50‐Unet model, which achieves accurate segmentation of fibers and matrix. In addition, adaptive grayscale thresholding combined with multi‐scale morphological pore elimination effectively suppresses the influence of pseudo‐cracks (defects or pores) while extracting cracks. Moreover, a KD‐Tree‐based crack connection algorithm module repairs micro‐crack fractures, significantly improving crack connectivity. The results demonstrate that the machine learning model achieves a segmentation accuracy of 97%. Following the pore elimination process, the crack line density, area density, and average width were significantly reduced from 18.8 mm/mm 2 , 7.2 mm 2 /cm 2 , and 6.8 µm to 1.1 mm/mm 2 , 0.2 mm 2 /cm 2 , and 2.2 µm, respectively. Subsequent to the crack connection procedure, the crack line density, area density, and total crack length increased from 1.1 mm/mm 2 , 0.23 mm 2 /cm 2 , and 1.8 cm to 1.6 mm/mm 2 , 0.31 mm 2 /cm 2 , and 2.1 cm, respectively. These findings validate the effectiveness of the proposed crack extraction framework in enabling precise crack quantification and offer a novel methodology for crack analysis in ceramic matrix composites.
- 7 November 2025
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 109 (1)
A machine learning‐based multi‐scale morphological approach for crack segmentation
To achieve quantitative analysis of cracks in different regions for C f /SiC composites, this study proposes an automated, multi‐scale crack segmentation and quantitative analysis framework for composites with complex backgrounds. This framework is based on the ResNet50‐Unet model, which achieves accurate segmentation of fibers and matrix. In addition, adaptive grayscale thresholding combined with multi‐scale morphological pore elimination effectively suppresses the influence of pseudo‐cracks (defects or pores) while extracting cracks. Moreover, a KD‐Tree‐based crack connection algorithm module repairs micro‐crack fractures, significantly improving crack connectivity. The results demonstrate that the machine learning model achieves a segmentation accuracy of 97%. Following the pore elimination process, the crack line density, area density, and average width were significantly reduced from 18.8 mm/mm 2 , 7.2 mm 2 /cm 2 , and 6.8 µm to 1.1 mm/mm 2 , 0.2 mm 2 /cm 2 , and 2.2 µm, respectively. Subsequent to the crack connection procedure, the crack line density, area density, and total crack length increased from 1.1 mm/mm 2 , 0.23 mm 2 /cm 2 , and 1.8 cm to 1.6 mm/mm 2 , 0.31 mm 2 /cm 2 , and 2.1 cm, respectively. These findings validate the effectiveness of the proposed crack extraction framework in enabling precise crack quantification and offer a novel methodology for crack analysis in ceramic matrix composites.
- 26 May 2025
- Published by Elsevier in Ceramics International
- Vol. 51 (22) , 36330-36339
Microstructural degradation mechanisms and high-temperature steam corrosion kinetics of domestic Cansas-Ⅲ SiC fibers
- 26 May 2025
- Published by Elsevier in Ceramics International
- Vol. 51 (22) , 36330-36339
Microstructural degradation mechanisms and high-temperature steam corrosion kinetics of domestic Cansas-Ⅲ SiC fibers
- 28 March 2025
- Published by Elsevier in Journal of the European Ceramic Society
- Vol. 45 (11)
Effect of molten NaCl on the wet oxidation behavior of Al2O3-modified SiC-B4C ceramics at 1300 ℃
- 28 March 2025
- Published by Elsevier in Journal of the European Ceramic Society
- Vol. 45 (11)
Effect of molten NaCl on the wet oxidation behavior of Al2O3-modified SiC-B4C ceramics at 1300 ℃
- 7 February 2024
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 21 (3) , 2183-2195
Mechanical properties and microstructure evolution of KD‐SA SiC f /BN/SiC CMCs oxidized at different temperatures
Silicon carbide fiber‐reinforced SiC ceramic matrix composites (SiC f /SiC CMCs) based on a domestic KD‐SA SiC fiber were exposed to a wet oxygen atmosphere for 135 h at 800, 1100, and 1300°C. The evolution of the microstructure and mechanical properties of SiC f /SiC CMCs have been systematically investigated following oxidation. For weight change, CMC‐1300 showed the greatest gain (0.394%), followed by CMC‐1100 (0.356%) and CMC‐800 (0.149%). The volatilization of boron oxide (B 2 O 3 ) combined with the slight oxidation of the SiC matrix at 800°C caused crack deflection and fiber pull‐out. The complete dissipation of the interphase could be found when the oxidation temperature increases to 1100°C, generated a fracture surface with brittle fracture characteristics. At 1300°C, crystalline SiO 2 hindered oxygen diffusion, with evidence of fiber pull‐out. Based on thermodynamic calculations and microscopic observations, we propose a mechanism to explain the thermal degradation of SiC f /SiC CMCs. This work offers valuable guidance for the fabrication of SiC f /SiC CMCs that are suitable for high‐temperature applications.
- 7 February 2024
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 21 (3) , 2183-2195
Mechanical properties and microstructure evolution of KD‐SA SiC f /BN/SiC CMCs oxidized at different temperatures
Silicon carbide fiber‐reinforced SiC ceramic matrix composites (SiC f /SiC CMCs) based on a domestic KD‐SA SiC fiber were exposed to a wet oxygen atmosphere for 135 h at 800, 1100, and 1300°C. The evolution of the microstructure and mechanical properties of SiC f /SiC CMCs have been systematically investigated following oxidation. For weight change, CMC‐1300 showed the greatest gain (0.394%), followed by CMC‐1100 (0.356%) and CMC‐800 (0.149%). The volatilization of boron oxide (B 2 O 3 ) combined with the slight oxidation of the SiC matrix at 800°C caused crack deflection and fiber pull‐out. The complete dissipation of the interphase could be found when the oxidation temperature increases to 1100°C, generated a fracture surface with brittle fracture characteristics. At 1300°C, crystalline SiO 2 hindered oxygen diffusion, with evidence of fiber pull‐out. Based on thermodynamic calculations and microscopic observations, we propose a mechanism to explain the thermal degradation of SiC f /SiC CMCs. This work offers valuable guidance for the fabrication of SiC f /SiC CMCs that are suitable for high‐temperature applications.
- 16 January 2024
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 107 (6) , 3701-3715
Corrosion behavior of precracked SiC f /SiC composites under 1200–1300°C Na 2 SO 4 ‐wet‐oxygen environment
SiC f /SiC composites, as promising materials for the hot‐section components of turbine engines, are susceptible to hot corrosion due to the steam environments. Especially, under rotational and thermal stress, numerous microcracks may be generated in the SiC f /SiC ceramic matrix, which can trigger the rapid invasion of corrosive gases and deteriorate the composite mechanical properties. Therefore, it is of great importance to investigate the degradation mechanisms of SiC f /SiC with precracks existing. Here, the corrosion behavior of precracked SiC f /SiC in the Na 2 SO 4 ‐wet‐oxygen environment was evaluated. By comparing mechanical evolution under different corrosion conditions, microfailure mechanisms of SiC f /SiC were revealed. The results indicate that brittle cracking of the matrix and oxidation erosion of fibers are the key factors in reducing the tensile strain of composites. Specifically, the composite damage resistance increases at 67 MPa‐1300°C. At this point, the prestress level is moderate and close to the matrix cracking limit. The prefabricated microcracks can be healed at 1300°C by liquid oxidation products, which hinders cracks bridging large‐scale. This study is conducive to a better understanding of failure mechanisms of SiC f /SiC in complex service environments.
- 16 January 2024
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 107 (6) , 3701-3715
Corrosion behavior of precracked SiC f /SiC composites under 1200–1300°C Na 2 SO 4 ‐wet‐oxygen environment
SiC f /SiC composites, as promising materials for the hot‐section components of turbine engines, are susceptible to hot corrosion due to the steam environments. Especially, under rotational and thermal stress, numerous microcracks may be generated in the SiC f /SiC ceramic matrix, which can trigger the rapid invasion of corrosive gases and deteriorate the composite mechanical properties. Therefore, it is of great importance to investigate the degradation mechanisms of SiC f /SiC with precracks existing. Here, the corrosion behavior of precracked SiC f /SiC in the Na 2 SO 4 ‐wet‐oxygen environment was evaluated. By comparing mechanical evolution under different corrosion conditions, microfailure mechanisms of SiC f /SiC were revealed. The results indicate that brittle cracking of the matrix and oxidation erosion of fibers are the key factors in reducing the tensile strain of composites. Specifically, the composite damage resistance increases at 67 MPa‐1300°C. At this point, the prestress level is moderate and close to the matrix cracking limit. The prefabricated microcracks can be healed at 1300°C by liquid oxidation products, which hinders cracks bridging large‐scale. This study is conducive to a better understanding of failure mechanisms of SiC f /SiC in complex service environments.