Effects of Isothermal Aging on Interfacial Microstructure and Shear Properties of Sn-4.5Sb-3.5Bi-0.1Ag Soldering with ENIG and ENEPIG Substrates
Open Access
Abstract
Sn–Sb system solders and ENIG/ENEPIG surface finish layers are commonly used in electronic products. To illustrate the thermal reliability evaluation of such solder joints, we studied the interfacial microstructure and shear properties of Sn-4.5Sb-3.5Bi-0.1Ag/ENIG and Sn-4.5Sb-3.5Bi-0.1Ag/ENEPIG solder joints after aging at 150 °C for 250, 500 and 1000 h. The results show that the intermetallic compound of Sn-4.5Sb-3.5Bi-0.1Ag/ENIG interface was more continuous and uniform compared with that of Sn-4.5Sb-3.5Bi-0.1Ag/ENEPIG interface after reflow. The thickness of the interfacial intermetallic compounds of the former was significantly thinner than that of the latter before and after aging. With extension of aging time, the former interface was stable, while obvious voids appeared at the interface of the latter after 500 h aging and significant fracture occurred after 1000 h aging. The shear tests proved that shear strength of solder joints decreased with increasing aging time. For the Sn-4.5Sb-3.5Bi-0.1Ag/ENEPIG joint after 1000 h aging, the fracture mode is ductile-brittle mixed type, which means fracture could occur at the solder matrix or the solder/IMC interface. For other samples of these two types of joints, ductile fracture occurred inside of the solder. The Sn-4.5Sb-3.5Bi-0.1Ag/ENIG solder joint was thermally more reliable than Sn-4.5Sb-3.5Bi-0.1Ag/ENEPIG.Keywords
Funding Information
- Hebei Provincial Key Research Projects (19250202D)
- National Natural Science Foundation of China (51875168)
- Natural Science Foundation of Hebei Province (E2020208083)
This publication has 28 references indexed in Scilit:
- Microstructure and impression creep behavior of lead-free Sn–5Sb solder alloy containing Bi and AgMaterials Science and Engineering: A, 2012
- Suppressing Ni3Sn4 formation in the Sn–Ag–Cu solder joints with Ni–P/Pd/Au surface finishMaterials Letters, 2011
- Evolution of CuSn intermetallics between molten SnAgCu solder and Cu substrateActa Materialia, 2008
- Indentation creep study of lead-free Sn–5%Sb solder alloyMaterials Science and Engineering: A, 2007
- Impression creep behavior of lead-free Sn–5Sb solder alloyMaterials Science and Engineering: A, 2007
- Shear strength and interfacial microstructure of Sn–Ag–xNi/Cu single shear lap solder jointsMaterials Science and Engineering: A, 2007
- Interfacial reaction of ENIG/Sn-Ag-Cu/ENIG sandwich solder joint during isothermal agingMicroelectronic Engineering, 2006
- High temperature aging study of intermetallic compound formation of Sn–3.5Ag and Sn–4.0Ag–0.5Cu solders on electroless Ni(P) metallizationJournal of Alloys and Compounds, 2006
- Correlation Between Chemical Reaction and Brittle Fracture Found in Electroless Ni(P)/immersion gold–solder InterconnectionJournal of Materials Research, 2005
- Six cases of reliability study of Pb-free solder joints in electronic packaging technologyMaterials Science and Engineering: R: Reports, 2002