Abstract
The mild to severe wear transition of Ti-6Al-4V titanium alloy was investigated. Thecorrelation between microstructure and wear micro-mechanisms was also studied.Hot swaging at 900 °C was performed on the as-cast samples and thereafter twodifferent solution treatments were applied on the swaged samples. The first treatmentwas applied at a temperature of 850 °C (below the -transus temperature) for gettinga bimodal structure (+), while the second treatment at 1050 °C was applied (abovethe -transus) for getting lamellar structure (). The solution treated lamellar structureresulted in ultimate strength of 1335 MPa and a hardness of 440 HV20 which aresignificantly superior to the bimodal structure. Wear behaviour of the studied Ti64alloy was investigated at different sliding speeds in the range of 0.5 to 2.5 m/s withan interval of 0.5 m/s. The mild to severe wear transition was obtained at 1.5 m/s.The lowest wear rate was reported for the samples solution treated at 1050 °C due totheir fine lamellae structure with high hardness. The worn surfaces of some selectedsamples were examined using SEM to determine the wear micro-mechanisms.

This publication has 22 references indexed in Scilit: