Khaled M. Ibrahim
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Khaled M. Ibrahim has a total of 30 co-authors. Here are the top co-authors by number of shared publications:
- Ashraf Bakkar
Department of Civil and Environmental Engineering, College of Engineering and Computers, Umm Al-Qura University, Al-Lith 28425, Saudi Arabia
3 shared publications - Hayam A. Aly
Central Metallurgical Research and Development Institute (CMRDI), P.O. Box 87, Helwan 11421, Egypt
3 shared publications Lothar Wagner
Institue of Materials Science and Engineering, TU Clausthal, Agricolastr. 6, 38678 Clausthal-Zellerfeld, Germany
3 shared publications- Mohamed M. El-Sayed Seleman
Department of Metallurgical and Materials Engineering, Faculty of Petroleum and Mining Engineering, Suez University, Suez 43221, Egypt
3 shared publications - Abdulaziz Salem Alghamdi
College of Engineering, University of Ha’il, Hail P.O. Box 2440, Saudi Arabia
2 shared publications - Badreddine Ayadi
Department of Mechanical Engineering, College of Engineering, University of Ha’il, Ha’il City 81451, Saudi Arabia
2 shared publications
Latest Publications
- Open Access
- 5 May 2026
- Published by Royal Society of Chemistry (RSC) in RSC Advances
- Vol. 16 (26) , 23848-23861
Effect of Si additions on the mechanical and electrochemical behavior of the as-casted Ti-15Mo alloy in simulated body fluid for biomedical applications
Titanium (Ti) and its alloys are preferred biomaterials for orthopedic and dental implants due to their excellent biocompatibility and corrosion resistance. However, the development of non-toxic β-Ti alloys with low elastic modulus, high strength, and superior corrosion resistance remains a key challenge for long-term implant applications. The Ti-15Mo alloy is a promising candidate due to its good biocompatibility and mechanical properties. This study investigates the influence of silicon additions (0–2 wt%) on the microstructure, mechanical properties, and corrosion behavior of as-cast Ti-15Mo-xSi alloys for biomedical applications. The corrosion behavior was investigated by potentiodynamic polarization and electrochemical impedance spectroscopy (EIS) at 37 °C in simulated body fluid (SBF). Moreover, the passive films formed on the surfaces of the alloys were examined using X-ray photoelectron spectroscopy analysis (XPS). The results indicated that Si additions refined the grain size and improved the mechanical properties. All alloys spontaneously formed a stable passive oxide layer. Crucially, the corrosion resistance improved systematically with Si content, as evidenced by a nobler open-circuit potential, a lower corrosion current density (reaching ∼1.03 × 10−7 A cm−2 for the 2 wt% Si alloy), and a higher passive film resistance. XPS confirmed that the passive film is primarily composed of TiO2, with the superior performance of the 2 wt% Si alloy attributed to a denser, more compact oxide layer enriched with protective silicon oxides. The Ti-15Mo-2Si alloy, combining high strength and exceptional corrosion resistance, emerges as a highly promising candidate for load-bearing surgical implants.
- 5 May 2026
- Published by Royal Society of Chemistry (RSC) in RSC Advances
- Vol. 16 (26) , 23848-23861
Open AccessEffect of Si additions on the mechanical and electrochemical behavior of the as-casted Ti-15Mo alloy in simulated body fluid for biomedical applications
Titanium (Ti) and its alloys are preferred biomaterials for orthopedic and dental implants due to their excellent biocompatibility and corrosion resistance. However, the development of non-toxic β-Ti alloys with low elastic modulus, high strength, and superior corrosion resistance remains a key challenge for long-term implant applications. The Ti-15Mo alloy is a promising candidate due to its good biocompatibility and mechanical properties. This study investigates the influence of silicon additions (0–2 wt%) on the microstructure, mechanical properties, and corrosion behavior of as-cast Ti-15Mo-xSi alloys for biomedical applications. The corrosion behavior was investigated by potentiodynamic polarization and electrochemical impedance spectroscopy (EIS) at 37 °C in simulated body fluid (SBF). Moreover, the passive films formed on the surfaces of the alloys were examined using X-ray photoelectron spectroscopy analysis (XPS). The results indicated that Si additions refined the grain size and improved the mechanical properties. All alloys spontaneously formed a stable passive oxide layer. Crucially, the corrosion resistance improved systematically with Si content, as evidenced by a nobler open-circuit potential, a lower corrosion current density (reaching ∼1.03 × 10−7 A cm−2 for the 2 wt% Si alloy), and a higher passive film resistance. XPS confirmed that the passive film is primarily composed of TiO2, with the superior performance of the 2 wt% Si alloy attributed to a denser, more compact oxide layer enriched with protective silicon oxides. The Ti-15Mo-2Si alloy, combining high strength and exceptional corrosion resistance, emerges as a highly promising candidate for load-bearing surgical implants.
- Open Access
Effect of the Si Content on the Dry and Wet Sliding Wear Behavior of the Developed Ti-15Mo-(0-2) Si Alloys for Biomedical Applications
The durability of a metallic biomaterial to withstand weight loss is a key factor in determining its service life and performance. Therefore, it is essential to create biomaterials with high wear resistance to ensure the biomaterial has a long service life. Thus, this study aims to explore the dry and wet sliding wear characteristics of the developed Ti-15Mo-xSi as-cast alloys (where x equals 0, 0.5, 1, 1.5, and 2 wt.%) in order to assess the impact of the Si addition on the microstructure, mechanical properties, and wear resistance and to consider them for biomedical applications. The wear experiments were conducted using a pin-on-desk wear testing machine at a load of 20 N and a sliding distance of 1000 m with and without applying simulated body fluid (SBF). Different techniques were utilized in the evaluation of the developed Ti-15Mo-xSi alloys. The results showed that significant grain refining was attained with the Si addition. The hardness, compressive strength, and wear resistance of the Ti-15Mo-xSi as-cast alloys increased with the increase in Si content. The Ti-15Mo-2Si as-cast alloy exhibited the highest dry and wet wear resistance of all the Ti-15Mo-xSi alloys. The worn surfaces were investigated, the roughness and main features were reported, and the wear mechanisms were also discussed.
Open AccessEffect of the Si Content on the Dry and Wet Sliding Wear Behavior of the Developed Ti-15Mo-(0-2) Si Alloys for Biomedical Applications
The durability of a metallic biomaterial to withstand weight loss is a key factor in determining its service life and performance. Therefore, it is essential to create biomaterials with high wear resistance to ensure the biomaterial has a long service life. Thus, this study aims to explore the dry and wet sliding wear characteristics of the developed Ti-15Mo-xSi as-cast alloys (where x equals 0, 0.5, 1, 1.5, and 2 wt.%) in order to assess the impact of the Si addition on the microstructure, mechanical properties, and wear resistance and to consider them for biomedical applications. The wear experiments were conducted using a pin-on-desk wear testing machine at a load of 20 N and a sliding distance of 1000 m with and without applying simulated body fluid (SBF). Different techniques were utilized in the evaluation of the developed Ti-15Mo-xSi alloys. The results showed that significant grain refining was attained with the Si addition. The hardness, compressive strength, and wear resistance of the Ti-15Mo-xSi as-cast alloys increased with the increase in Si content. The Ti-15Mo-2Si as-cast alloy exhibited the highest dry and wet wear resistance of all the Ti-15Mo-xSi alloys. The worn surfaces were investigated, the roughness and main features were reported, and the wear mechanisms were also discussed.
- Open Access
Effect of Si Content on the Thermal Expansion of Ti15Mo(0–2 Si) Biomaterial Alloys during Different Heating Rates
Thermal expansion measurements were used to characterize phase transformations in metastable β-Ti alloys (Ti15MoxSi) without and with various Si additions (where x = 0, 0.5, 1.0, 1.5, and 2 in wt.%) during linear heating at two heating rates of 5 and 10 °C/min up to 850 °C. For this study, five alloys were developed and examined in terms of their presence phases, microstructures, and starting and final transformation temperatures. According to the results, all of the as-cast samples primarily include an equiaxed β-Ti phase. The influence of phase transformation on the material dimensions was discussed and compared with the variations in Si contents. The transformation was investigated using a dilatometric technique for the developed alloys during continuous heating and cooling. The dilatometric curve of heating revealed two distinct reflection points as the heating temperature increased. The starting transformation temperature (Ts) to obtain the ω-phase was reported at 359 °C without Si addition; whereas the final transformation temperature (Tf) of the dissolution of α-phase was obtained at 572 °C at a heating rate of 10 °C/min. At 2 wt.% Si, the first derivative curves reported Ts and Tf transforming temperatures of 314–565 °C (at a 5 °C/min heating rate) and 270–540 °C (at a 10 °C/min heating rate), respectively. The Ts and Tf transforming temperatures were significantly decreased with Si additions, which decreased the β-transus temperature. Moreover, the thermal expansion coefficient curves of the investigated alloys without and with 2 wt.% Si were studied. The transformation heating curves have an S-shaped pattern, according to the results.
Open AccessEffect of Si Content on the Thermal Expansion of Ti15Mo(0–2 Si) Biomaterial Alloys during Different Heating Rates
Thermal expansion measurements were used to characterize phase transformations in metastable β-Ti alloys (Ti15MoxSi) without and with various Si additions (where x = 0, 0.5, 1.0, 1.5, and 2 in wt.%) during linear heating at two heating rates of 5 and 10 °C/min up to 850 °C. For this study, five alloys were developed and examined in terms of their presence phases, microstructures, and starting and final transformation temperatures. According to the results, all of the as-cast samples primarily include an equiaxed β-Ti phase. The influence of phase transformation on the material dimensions was discussed and compared with the variations in Si contents. The transformation was investigated using a dilatometric technique for the developed alloys during continuous heating and cooling. The dilatometric curve of heating revealed two distinct reflection points as the heating temperature increased. The starting transformation temperature (Ts) to obtain the ω-phase was reported at 359 °C without Si addition; whereas the final transformation temperature (Tf) of the dissolution of α-phase was obtained at 572 °C at a heating rate of 10 °C/min. At 2 wt.% Si, the first derivative curves reported Ts and Tf transforming temperatures of 314–565 °C (at a 5 °C/min heating rate) and 270–540 °C (at a 10 °C/min heating rate), respectively. The Ts and Tf transforming temperatures were significantly decreased with Si additions, which decreased the β-transus temperature. Moreover, the thermal expansion coefficient curves of the investigated alloys without and with 2 wt.% Si were studied. The transformation heating curves have an S-shaped pattern, according to the results.
- Open Access
Microstructure and Mechanical Performance of Tin-Based Babbitt Alloy Containing Iron Oxide and Silica Nanoparticles
Iron oxide and silica nanoparticles were individually incorporated in tin-based Babbitt alloy and combined to prepare a novel class of nanocomposites for bearing material applications. The route of liquid metallurgy in combination with the stirring technique was adopted to manufacture nanocomposites. Microstructural evolution and mechanical property evaluation were performed by optical and electron microscopy, EDS, hardness, compression, and wear tests. The morphology of the Cu6Sn5 phase was changed from elongated to spherical in the microstructures of nanocomposites. The solitary addition of 0.5 wt% iron oxide nanoparticles improved the hardness and compressive strength but adversely affected the wear properties by increasing the weight loss and friction coefficient value. In contrast, the addition of 0.5 wt% silica nanoparticles could not significantly increase the hardness and compressive strength but it could improve the tribological properties by reducing the weight loss and friction coefficient value. Tin-based Babbitt alloy showed a compressive strength of 89.22 ± 0.50 MPa after the addition of 0.5 wt% iron oxide showing a rise of ~11%. The combined effect of the addition of both types of nanoparticles showed considerable results, i.e., a rise of ~7.9% (86.75 ± 0.68 MPa). The balanced approach of incorporating dual reinforcements of 0.25 wt% iron oxide and 0.25 wt% silica nanoparticles intermediately improved the hardness, compressive strength, and decreased weight loss.
Open AccessMicrostructure and Mechanical Performance of Tin-Based Babbitt Alloy Containing Iron Oxide and Silica Nanoparticles
Iron oxide and silica nanoparticles were individually incorporated in tin-based Babbitt alloy and combined to prepare a novel class of nanocomposites for bearing material applications. The route of liquid metallurgy in combination with the stirring technique was adopted to manufacture nanocomposites. Microstructural evolution and mechanical property evaluation were performed by optical and electron microscopy, EDS, hardness, compression, and wear tests. The morphology of the Cu6Sn5 phase was changed from elongated to spherical in the microstructures of nanocomposites. The solitary addition of 0.5 wt% iron oxide nanoparticles improved the hardness and compressive strength but adversely affected the wear properties by increasing the weight loss and friction coefficient value. In contrast, the addition of 0.5 wt% silica nanoparticles could not significantly increase the hardness and compressive strength but it could improve the tribological properties by reducing the weight loss and friction coefficient value. Tin-based Babbitt alloy showed a compressive strength of 89.22 ± 0.50 MPa after the addition of 0.5 wt% iron oxide showing a rise of ~11%. The combined effect of the addition of both types of nanoparticles showed considerable results, i.e., a rise of ~7.9% (86.75 ± 0.68 MPa). The balanced approach of incorporating dual reinforcements of 0.25 wt% iron oxide and 0.25 wt% silica nanoparticles intermediately improved the hardness, compressive strength, and decreased weight loss.
- Open Access
Influence of Microstructure and Alloy Composition on the Machinability of α/β Titanium Alloys
A comparative study was conducted for the machining of two α/β titanium alloys, namely Ti-6Al-4V (Ti64) and Ti-6Al-7Nb (Ti67), using wire electric discharge machining (WEDM). The influence of cutting speed and cutting mode on the machined surfaces in terms of surface roughness (Ra), recast layer (RL), and micro-hardness have been evaluated. Rough cut (RC) mode at a cutting speed of 50 µm/s resulted in thermal damage; Ra was equal to 5.68 ± 0.44 and 4.52 ± 0.35 µm for Ti64 and Ti67, respectively. Trim-cut mode using seven cuts (TRC-VII) at the same speed decreased the Ra to 1.02 ± 0.20 µm for Ti64 and 0.92 ± 0.10 µm for Ti67. At 100 µm/s, Ra reduced from 2.34 ± 0.28 µm to 0.88 ± 0.12 µm (Ti64), and from 1.42 ± 0.15 µm to 0.90 ± 0.08µm (Ti67) upon changing from TRC-III to TRC-VII. Furthermore, a thick recast layer of 30 ± 0.93 µm for Ti64 and 14 ± 0.68 µm for Ti67 was produced using the rough mode, while TRC-III and TRC-VII modes produced layers of 12 ± 1.31 µm and 5 ± 0.72 µm for Ti64 and Ti67, respectively. Moreover, rough cut and trim cut modes of WEDM played a significant role in promoting the surface hardness of Ti64 and Ti67. By employing the Response Surface Methodology, it was found that the machining mode followed by cutting speed and the interaction between them are the most influential parameters on surface roughness. Finally, mathematical models correlating machining parameters to surface roughness were successfully developed. The results strongly promote the trim-cut mode of WEDM as a promising machining route for two-phase titanium alloys.
Open AccessInfluence of Microstructure and Alloy Composition on the Machinability of α/β Titanium Alloys
A comparative study was conducted for the machining of two α/β titanium alloys, namely Ti-6Al-4V (Ti64) and Ti-6Al-7Nb (Ti67), using wire electric discharge machining (WEDM). The influence of cutting speed and cutting mode on the machined surfaces in terms of surface roughness (Ra), recast layer (RL), and micro-hardness have been evaluated. Rough cut (RC) mode at a cutting speed of 50 µm/s resulted in thermal damage; Ra was equal to 5.68 ± 0.44 and 4.52 ± 0.35 µm for Ti64 and Ti67, respectively. Trim-cut mode using seven cuts (TRC-VII) at the same speed decreased the Ra to 1.02 ± 0.20 µm for Ti64 and 0.92 ± 0.10 µm for Ti67. At 100 µm/s, Ra reduced from 2.34 ± 0.28 µm to 0.88 ± 0.12 µm (Ti64), and from 1.42 ± 0.15 µm to 0.90 ± 0.08µm (Ti67) upon changing from TRC-III to TRC-VII. Furthermore, a thick recast layer of 30 ± 0.93 µm for Ti64 and 14 ± 0.68 µm for Ti67 was produced using the rough mode, while TRC-III and TRC-VII modes produced layers of 12 ± 1.31 µm and 5 ± 0.72 µm for Ti64 and Ti67, respectively. Moreover, rough cut and trim cut modes of WEDM played a significant role in promoting the surface hardness of Ti64 and Ti67. By employing the Response Surface Methodology, it was found that the machining mode followed by cutting speed and the interaction between them are the most influential parameters on surface roughness. Finally, mathematical models correlating machining parameters to surface roughness were successfully developed. The results strongly promote the trim-cut mode of WEDM as a promising machining route for two-phase titanium alloys.
- Open Access
Influence of Pre-Tinning Process on Coating Morphology and Interface Structure of Low Carbon Steel Dipped in Molten 6061 Al Alloy
Pre-treated low carbon steel specimens with flux or flux + tin mixture were coated by hot-dip aluminizing process. Al alloy (6061) was melted and hold at 750 °C. Fluxed and pre-tinned low carbon steel samples were dipped in a molten bath for time intervals of 0.5, 1, 2.5 and 3.5 min. Applying double coating processes via tinning-aluminizing techniques facilitated the formation of Fe-Al intermetallic interface and increasing the thickness of homogenous coating layer over the substrate material. The presence of Sn facilitates to great extent the formation of a better interlayer-free bond of residual flux and/or oxides. The fluxed–dipped steel substrates have inhomogeneous distribution of Al alloy coating as well as an interface with residual flux and oxides for dipping time up to 2.5 min. A homogenous distribution with good thickness morphology of the Al alloy coating and homogeneous thin intermetallic interface was achieved for tinned steel substrate at all applied dipping times. The comparison between the pre-tinning and pre-fluxing processes on steel substrates showed a significant effect of tinning over fluxing treatment acting on the thickness layer of Al-coating and interface using a short time dipping. For dipping time up to 2.5 min, the hardness of pre-tinning substrates is greater than that of fluxed ones due to the presence of residual flux and void interface in fluxed steel.
Open AccessInfluence of Pre-Tinning Process on Coating Morphology and Interface Structure of Low Carbon Steel Dipped in Molten 6061 Al Alloy
Pre-treated low carbon steel specimens with flux or flux + tin mixture were coated by hot-dip aluminizing process. Al alloy (6061) was melted and hold at 750 °C. Fluxed and pre-tinned low carbon steel samples were dipped in a molten bath for time intervals of 0.5, 1, 2.5 and 3.5 min. Applying double coating processes via tinning-aluminizing techniques facilitated the formation of Fe-Al intermetallic interface and increasing the thickness of homogenous coating layer over the substrate material. The presence of Sn facilitates to great extent the formation of a better interlayer-free bond of residual flux and/or oxides. The fluxed–dipped steel substrates have inhomogeneous distribution of Al alloy coating as well as an interface with residual flux and oxides for dipping time up to 2.5 min. A homogenous distribution with good thickness morphology of the Al alloy coating and homogeneous thin intermetallic interface was achieved for tinned steel substrate at all applied dipping times. The comparison between the pre-tinning and pre-fluxing processes on steel substrates showed a significant effect of tinning over fluxing treatment acting on the thickness layer of Al-coating and interface using a short time dipping. For dipping time up to 2.5 min, the hardness of pre-tinning substrates is greater than that of fluxed ones due to the presence of residual flux and void interface in fluxed steel.
- 30 November 2021
- Published by Springer Nature in International Journal of Metalcasting
- Vol. 16 (4) , 1693-1708
Fatigue Properties and Simulation of Thin Wall ADI and IADI Castings
- 30 November 2021
- Published by Springer Nature in International Journal of Metalcasting
- Vol. 16 (4) , 1693-1708
Fatigue Properties and Simulation of Thin Wall ADI and IADI Castings
- Open Access
- 1 April 2016
- Published by Egyptian Knowledge Bank in The International Conference on Applied Mechanics and Mechanical Engineering
- Vol. 17 (17) , 1-11
INFLUENCE OF MICROSTRUCTURE FEATURES ON WEAR BEHAVIOUR OF Ti-64 TITANIUM ALLOY
The mild to severe wear transition of Ti-6Al-4V titanium alloy was investigated. Thecorrelation between microstructure and wear micro-mechanisms was also studied.Hot swaging at 900 °C was performed on the as-cast samples and thereafter twodifferent solution treatments were applied on the swaged samples. The first treatmentwas applied at a temperature of 850 °C (below the -transus temperature) for gettinga bimodal structure (+), while the second treatment at 1050 °C was applied (abovethe -transus) for getting lamellar structure (). The solution treated lamellar structureresulted in ultimate strength of 1335 MPa and a hardness of 440 HV20 which aresignificantly superior to the bimodal structure. Wear behaviour of the studied Ti64alloy was investigated at different sliding speeds in the range of 0.5 to 2.5 m/s withan interval of 0.5 m/s. The mild to severe wear transition was obtained at 1.5 m/s.The lowest wear rate was reported for the samples solution treated at 1050 °C due totheir fine lamellae structure with high hardness. The worn surfaces of some selectedsamples were examined using SEM to determine the wear micro-mechanisms.
- 1 April 2016
- Published by Egyptian Knowledge Bank in The International Conference on Applied Mechanics and Mechanical Engineering
- Vol. 17 (17) , 1-11
Open AccessINFLUENCE OF MICROSTRUCTURE FEATURES ON WEAR BEHAVIOUR OF Ti-64 TITANIUM ALLOY
The mild to severe wear transition of Ti-6Al-4V titanium alloy was investigated. Thecorrelation between microstructure and wear micro-mechanisms was also studied.Hot swaging at 900 °C was performed on the as-cast samples and thereafter twodifferent solution treatments were applied on the swaged samples. The first treatmentwas applied at a temperature of 850 °C (below the -transus temperature) for gettinga bimodal structure (+), while the second treatment at 1050 °C was applied (abovethe -transus) for getting lamellar structure (). The solution treated lamellar structureresulted in ultimate strength of 1335 MPa and a hardness of 440 HV20 which aresignificantly superior to the bimodal structure. Wear behaviour of the studied Ti64alloy was investigated at different sliding speeds in the range of 0.5 to 2.5 m/s withan interval of 0.5 m/s. The mild to severe wear transition was obtained at 1.5 m/s.The lowest wear rate was reported for the samples solution treated at 1050 °C due totheir fine lamellae structure with high hardness. The worn surfaces of some selectedsamples were examined using SEM to determine the wear micro-mechanisms.
- Open Access
- 29 April 2014
- Published by Hindawi Limited in Journal of Metallurgy
- Vol. 2014, 1-9
Heat Treatment in High Chromium White Cast Iron Ti Alloy
The influence of heat treatment on microstructure and mechanical properties of high chromium white cast iron alloyed with titanium was investigated. The austenitizing temperatures of 980°C and 1150°C for 1 hour each followed by tempering at 260°C for 2 hours have been performed and the effect of these treatments on wear resistance/impact toughness combination is reported. The microstructure of irons austenitized at 1150°C showed a fine precipitate of secondary carbides (M6C23) in a matrix of eutectic austenite and eutectic carbides (M7C3). At 980°C, the structure consisted of spheroidal martensite matrix, small amounts of fine secondary carbides, and eutectic carbides. Titanium carbides (TiC) particles with cuboidal morphology were uniformly distributed in both matrices. Irons austenitized at 980°C showed relatively higher tensile strength compared to those austenitized at 1150°C, while the latter showed higher impact toughness. For both cases, optimum tensile strength was reported for the irons alloyed with 1.31% Ti, whereas maximum impact toughness was obtained for the irons without Ti-addition. Higher wear resistance was obtained for the samples austenitized at 980°C compared to the irons treated at 1150°C. For both treatments, optimum wear resistance was obtained with 1.3% Ti.
- 29 April 2014
- Published by Hindawi Limited in Journal of Metallurgy
- Vol. 2014, 1-9
Open AccessHeat Treatment in High Chromium White Cast Iron Ti Alloy
The influence of heat treatment on microstructure and mechanical properties of high chromium white cast iron alloyed with titanium was investigated. The austenitizing temperatures of 980°C and 1150°C for 1 hour each followed by tempering at 260°C for 2 hours have been performed and the effect of these treatments on wear resistance/impact toughness combination is reported. The microstructure of irons austenitized at 1150°C showed a fine precipitate of secondary carbides (M6C23) in a matrix of eutectic austenite and eutectic carbides (M7C3). At 980°C, the structure consisted of spheroidal martensite matrix, small amounts of fine secondary carbides, and eutectic carbides. Titanium carbides (TiC) particles with cuboidal morphology were uniformly distributed in both matrices. Irons austenitized at 980°C showed relatively higher tensile strength compared to those austenitized at 1150°C, while the latter showed higher impact toughness. For both cases, optimum tensile strength was reported for the irons alloyed with 1.31% Ti, whereas maximum impact toughness was obtained for the irons without Ti-addition. Higher wear resistance was obtained for the samples austenitized at 980°C compared to the irons treated at 1150°C. For both treatments, optimum wear resistance was obtained with 1.3% Ti.
- Open Access
- 25 February 2014
- Published by Hindawi Limited in Journal of Metallurgy
- Vol. 2014, 1-6
Characteristics of Anodized Layer in Investment Cast Ni50Ti50 Shape Memory Alloy
NiTi shape memory alloys are promising implant materials due to their shape memory effect and super elasticity. In the current study, some Ni50Ti50 (mass %) SMAs samples were prepared by investment casting. These samples were then anodized and thermally treated to improve the surface properties. A fully saturated oxide layer was obtained. The structure and hardness properties of the anodized surfaces were then investigated. A hard porous layer with no free Ni atoms could be obtained which can be used as prebiomimetic surface for biological application.
- 25 February 2014
- Published by Hindawi Limited in Journal of Metallurgy
- Vol. 2014, 1-6
Open AccessCharacteristics of Anodized Layer in Investment Cast Ni50Ti50 Shape Memory Alloy
NiTi shape memory alloys are promising implant materials due to their shape memory effect and super elasticity. In the current study, some Ni50Ti50 (mass %) SMAs samples were prepared by investment casting. These samples were then anodized and thermally treated to improve the surface properties. A fully saturated oxide layer was obtained. The structure and hardness properties of the anodized surfaces were then investigated. A hard porous layer with no free Ni atoms could be obtained which can be used as prebiomimetic surface for biological application.