Abstract
A fluidized bed reactor has been developed which uses a two-step thermochemical water splitting process with a peak hydrogen production rate of 47 Ncm3/min.gFe at an oxidation temperature of 850 °C. Of particular interest, is that a mixture of iron and zirconia powder is fluidized during the oxidation reaction using a steam mass flux of 58 g/min-cm2. The zirconia powder serves to virtually eliminate iron powder sintering while maintaining a high reaction rate. The iron/zirconia powder is mixed in a ratio of 1:2 by apparent volume and has a mass ratio of 1:1. Both iron and zirconia particles are sieved to sizes ranging from 125 μm to 355 μm. The efficacy of zirconia as a sintering inhibitor was found to be dependent on the iron and zirconia mean particle size, particle size distribution and iron/zirconia apparent volume ratio. At 650 °C, the oxidation of iron powder with a mean particle size of 100 μm and a wide particle size distribution (40–250 μm) mixed with 44 μm zirconia powder with an iron/zirconia apparent volume ratio of 1:1 results in 75–90% sintering. In all cases, when iron is mixed with zirconia, the hydrogen production rate is not affected when compared with the pure iron case assuming an equivalent mass of iron is in the mixture. When iron powder is mixed with zirconia, both with a narrow particle size distribution (125–355 μm), the first oxidation step results in 3–7% sintering when the reactions are carried out at temperatures ranging between 840 and 895 °C. The hydrogen fractional yield is high (94–97%). For subsequent redox reactions, the macroscopic sintering is totally eliminated at 867 and 895 °C, although the hydrogen fractional yield decreases to 27 and 33%, respectively. It is demonstrated that mixing iron with zirconia in an equivalent mass ratio and similar particle size range can eliminate macroscopic sintering in a fluidized bed reactor at elevated temperatures up to 895 °C.Keywords
This publication has 16 references indexed in Scilit:
- Production and Enhancement of Hydrogen From Water: A ReviewJournal of Energy Resources Technology, 2012
- Thermal Pyrolysis of Polyethylene in Fluidized Beds: Review of the Influence of Process Parameters on Product DistributionJournal of Energy Resources Technology, 2012
- Features of solar thermochemical redox cycles for hydrogen production from water as a function of reactants’ main characteristicsInternational Journal of Hydrogen Energy, 2011
- Life Cycle Assessment of Hydrogen Production Using Nuclear Energy: An Application Based on Thermochemical Water SplittingJournal of Energy Resources Technology, 2010
- Solar Hydrogen Production Integrating Low-Grade Solar Thermal Energy and Methanol Steam ReformingJournal of Energy Resources Technology, 2009
- Iron-Containing Yttria-Stabilized Zirconia System For Two-Step Thermochemical Water SplittingJournal of Solar Energy Engineering, 2007
- Thermochemical hydrogen production by a redox system of ZrO2-supported Co(II)-ferriteSolar Energy, 2005
- The Case for Hydrogen in a Carbon Constrained WorldJournal of Energy Resources Technology, 2005
- Solar hydrogen production via a two-step water-splitting thermochemical cycle based on Zn/ZnO redox reactionsInternational Journal of Hydrogen Energy, 2002
- Comparative experimental investigations of the water-splitting reaction with iron oxide Fe1−yO and iron manganese oxides (Fe1−xMnx)1−yOSolid State Ionics, 1995