Decay of softwood in archaeological wooden artifacts
- 21 March 2016
- journal article
- research article
- Published by Maney Publishing in Studies in Conservation
- Vol. 62 (2) , 83-95
Abstract
Hardwoods and softwoods were used side by side throughout Egyptian history, and importing softwoods that had an attractive color and texture was common. Over the decades, artifacts based on hardwoods and softwoods underwent deterioration phenomena, sometimes reaching either a level of brittleness or turning into a wood powder that may easily crumble. These levels of decay/degradation are often difficult to handle in terms of conservation treatments. To study or identify the reasons for decay has always been a point of interest for conservation purposes, but to assess decay and choose an appropriate treatment according to the state of preservation for the sake of keeping an artifact intact has become a subject of major importance. It is difficult at times to understand the deterioration process, because hardwoods and softwoods are different in structure, properties, and chemical composition. For this preliminary study, decayed samples from three commonly used softwood types, cypress (Cupressus sp.), cedar (Cedrus sp.), and pine (Pinus sp.), were identified and chosen. Scanning electron microscopy (SEM) of the samples indicated the degree of decay. Decayed and non-aged samples of the same wood type were analyzed using Fourier transform infrared spectroscopy (FTIR), and all the major carbohydrate and lignin bands were recorded. The strong hydrogen bonded (O–H) stretching absorption associated with water linked by hydrogen bonds to the –OH groups of cellulose and hemicelluloses in all decayed samples increased with decay. The brown powdery, fragile samples that had been evidently affected by microbial decay had a higher amount of lignin. The lignin/carbohydrate ratio was calculated and results compared. The increase of either lignin percentage or extractives in some of the samples had caused a darkening of color in both cypress and cedar samples, but the pine sample did not have the same texture and appearance. In cases where the lignin percentage decreased the samples had changed to a slightly lighter color. FTIR results explained the decay phenomena observed in SEM micrographs and helped assess wood decay and also confirmed results that had been previously obtained while applying traditional chemical analysis on wood.Keywords
This publication has 26 references indexed in Scilit:
- Modeling color and chemical changes on normal and red heart beech wood by reflectance spectrophotometry, Fourier Transform Infrared spectroscopy and hyperspectral imagingPolymer Degradation and Stability, 2015
- Changing research trends in the field of archaeological wood at the Conservation Department, Faculty of Archaeology, Cairo UniversityStudies in Conservation, 2014
- Light-induced color changes and chemical modification of treated and untreated chestnut wood surfaceStudies in Conservation, 2014
- How spectroscopy and microspectroscopy of degraded wood contribute to understand fungal wood decayApplied Microbiology and Biotechnology, 2012
- Characterisation of archaeological wood: A case study on the deterioration of a coffinMicrochemical Journal, 2009
- Comparison of the hygroscopic behaviour of 205-year-old and recently cut juvenile wood fromPinus sylvestrisL.Annals of Forest Science, 2006
- Nitrogen cycling by wood decomposing soft-rot fungi in the “King Midas tomb,” Gordion, TurkeyProceedings of the National Academy of Sciences, 2001
- Anatomical invesigation of 4,000-years old cedrus libani wood remains from EgyptActa Botanica Hungarica, 2001
- Assessment of Deterioration in Archaeological Wood from Ancient EgyptJournal of the American Institute for Conservation, 1994
- Infrared Studies of Wood Weathering. Part I: SoftwoodsApplied Spectroscopy, 1991