Effect of binder composition on densification, microstructural development, and quasi-static and dynamic compressive response of 92 wt.% tungsten heavy alloys containing Al and/or Ti
Authors:
- Mohsen RaziMRMohsen Razi
- Gholamreza EbrahimiGEGholamreza Ebrahimi
- Mohammad Hassan FarshidiMFMohammad Hassan Farshidi
- Amir MomeniAMAmir Momeni
- Hassan NajafiHNHassan Najafi
Preprint
- 24 July 2026
- preprint
- Published by Elsevier in SSRN Electronic Journal
Abstract
Binder composition governs liquid-phase sintering and mechanical response in tungsten heavy alloys. Three 92 wt.% tungsten heavy alloys with Ni-Co-Fe-Al-Ti, Ni-Fe-Al, and Ni-free Co-Fe-Ti binders, designated W-NCFAT, W-NFA, and W-CFT, were produced by elemental powder milling, cold isostatic pressing, liquid-phase sintering at 1425 and 1455 °C under a controlled vacuum-H2-Ar atmosphere sequence, and vacuum dehydrogenation. Densification, tungsten grain morphology, binder continuity, elemental partitioning, contiguity, hardness, and compressive behavior were compared under identical processing conditions. The Ni-containing alloys reached 95.8-97.0% relative density and developed rounded tungsten grains separated by continuous metallic binder regions. W-CFT increased from 78.1% relative density at 1425 °C to 90.4% at 1455 °C, but retained substantial porosity, incomplete grain spheroidization, and discontinuous binder regions. W-NCFAT showed the highest hardness and reached a peak true compressive stress of 1255.4 MPa under quasi-static loading. W-NFA showed a lower peak stress but sustained a final true strain of 0.589 and a higher deformation energy density. In a representative split Hopkinson pressure bar comparison at approximately 2 × 10³ s⁻¹, W-NFA reached a corrected true stress of 1020.7 MPa and remained intact to a final true strain of 0.344, whereas W-NCFAT reached 832.9 MPa at 0.065 before rapid load loss and fragmentation. EDS and XRD indicated continuous Ni-containing metallic binders, discrete Al/Ti-enriched oxygen-bearing constituents, dominant BCC tungsten, and weak reflections consistent with an FCC binder. Effective Al/Ti-containing binder modification therefore required sufficient Ni-assisted liquid-phase activity.Keywords
This publication has 25 references indexed in Scilit:
- Microstructure evolutions of liquid phase sintered W-Ni-Fe alloy under gravityInternational Journal of Refractory Metals and Hard Materials, 2025
- Understanding the effect of NiB/Co ratio on densification, distortion and compressive deformation of 90W-xNiB-2Fe-(8 – x)Co heavy alloysInternational Journal of Refractory Metals and Hard Materials, 2025
- Recent Advancement in Tungsten Heavy Alloy Processing for Different Industrial ApplicationsJournal of Materials Engineering and Performance, 2024
- The effect of pressure and temperature on the properties of 88 W-10Ni-2Mn tungsten heavy alloy produced by cold press methodInternational Journal of Refractory Metals and Hard Materials, 2024
- Systematic investigation of microstructure, distortion, mechanical and thermal properties of NiB and ZrB2-modified 90W-6Ni-4Co alloysInternational Journal of Refractory Metals and Hard Materials, 2024
- Tungsten heavy alloy: Nano-crystallinity and alloying induced low temperature sintering, microstructure and mechanical propertiesInternational Journal of Refractory Metals and Hard Materials, 2024
- Sintered tungsten heavy alloys: Review of microstructure, strength, densification, and distortionInternational Journal of Refractory Metals and Hard Materials, 2022
- “Self-sharpening” tungsten high-entropy alloyActa Materialia, 2020
- Effects of Ni/Co ratio and mechanical alloying on characteristics and sintering behavior of W-Ni-Co tungsten heavy alloysJournal of Alloys and Compounds, 2017
- Grain growth in liquid-phase-sintered W-Mo-Ni-Fe alloysJournal of the Less Common Metals, 1991