Amir Momeni
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Amir Momeni has a total of 88 co-authors. Here are the top co-authors by number of shared publications:
- Mohammadreza Mokhtare
Hamedan University of Technology
7 shared publications - Saeed Sadeghpour
Univ Oulu, Ctr Adv Steels Res Mat & Mech Engn, Oulu 90014, Finland
6 shared publications Haniyeh Moradjoo Hamedani
5 shared publications- Gholam Reza Ebrahimi
Department of Materials Science and Engineering, Faculty of Engineering, Ferdowsi University of Mashhad, Mashhad, Iran
4 shared publications Behzad Tolaminejad
3 shared publicationsHamid Keshmiri
‡Esfarayen Steel Complex, Esfarayen 1589673711, Iran
3 shared publications
Latest Publications
- Open Access
- 17 October 2026
- Published by Elsevier in SSRN Electronic Journal
Design and Deformation Mechanisms of a Novel TWIP High Entropy Steel
In this research, a novel twinning-induced plasticity (TWIP) high entropy steel (HES) was designed and subjected to uniaxial compression tests. Three stages were identified in the work hardening rate (q)-strain (e) curve. Stage I, appearing in the strain range eys<e£0.028 and characterized by a decrease in q, was governed by rapid dislocation multiplication and slip. Stage II, appearing in the strain range 0.028<e£0.034, was characterized by an increase in q value, due to the formation of initial twins, thereby obstructing dislocations. Stage III was characterized by a gradual decrease in q, in the strain range of 0.1-0.4. In stage III, successive twinning waves occurred in the form of small "work-hardening bumps". With increasing applied strain, the fraction of twin boundaries first decreased to 16 % (at e=0.1), due to the elongation of austenite grains and the partial transformation of annealing twins into high-angle boundaries, and then increased to 42 % (at e=0.4). It was found that the twinning fraction-strain curve followed a sigmoidal trend; consequently, saturation was expected to occur at strains exceeding 0.4. Based on the experimental data and the observed sigmoidal trend, an Avrami-type function was proposed to describe the dependence of twinning fraction on the applied strain.
- 17 October 2026
- Published by Elsevier in SSRN Electronic Journal
Open AccessDesign and Deformation Mechanisms of a Novel TWIP High Entropy Steel
In this research, a novel twinning-induced plasticity (TWIP) high entropy steel (HES) was designed and subjected to uniaxial compression tests. Three stages were identified in the work hardening rate (q)-strain (e) curve. Stage I, appearing in the strain range eys<e£0.028 and characterized by a decrease in q, was governed by rapid dislocation multiplication and slip. Stage II, appearing in the strain range 0.028<e£0.034, was characterized by an increase in q value, due to the formation of initial twins, thereby obstructing dislocations. Stage III was characterized by a gradual decrease in q, in the strain range of 0.1-0.4. In stage III, successive twinning waves occurred in the form of small "work-hardening bumps". With increasing applied strain, the fraction of twin boundaries first decreased to 16 % (at e=0.1), due to the elongation of austenite grains and the partial transformation of annealing twins into high-angle boundaries, and then increased to 42 % (at e=0.4). It was found that the twinning fraction-strain curve followed a sigmoidal trend; consequently, saturation was expected to occur at strains exceeding 0.4. Based on the experimental data and the observed sigmoidal trend, an Avrami-type function was proposed to describe the dependence of twinning fraction on the applied strain.
- Open Access
- 26 September 2026
- Published by Elsevier in SSRN Electronic Journal
Characterization of a Novel Multicomponent High Entropy Steel with TWIP behavior: Design and Deformation behavior
In this research, a novel twinning-induced plasticity (TWIP) high entropy steel (HES) was designed using an approach combining thermodynamic criteria and multivariate optimization. The chemical composition was tailored to simultaneously satisfy the high entropy criterion, promote the formation of a single-phase fcc solid solution, and maintain the stacking fault energy within the appropriate range for the activation of the TWIP effect during deformation. Uniaxial compression tests were performed at strain levels of 0.1, 0.2, 0.3, and 0.4 and the corresponding microstructural evolutions were studied using optical microscopy and SEM-EBSD methods. The compressive yield stress of the material was determined to be 350 MPa. This value is at the upper limit of the yield stress of conventional TWIP steels. Three stages were identified in the work hardening rate ()-applied strain () curve. Stage I, appearing in the strain range ys<0.028 and characterized by a decrease in , was governed by rapid dislocation multiplication and slip. Stage II, appearing in the strain range 0.028<0.034, was characterized by an increase in value, due to the formation of initial twins, thereby obstructing dislocations. Stage III was characterized by a gradual decrease in , in the strain range of 0.1-0.4. In stage III, successive twinning waves occurred in the form of small "work-hardening bumps". The EBSD results confirmed that in the annealed (undeformed) sample, 39 % of the boundaries were annealing twin boundaries, and the rest were high-angle grain boundaries. With increasing applied strain, the fraction of twin boundaries first decreased to 16 % (at =0.1), due to the elongation of austenite grains and the partial transformation of annealing twins into high-angle boundaries, and then increased to 42 % (at =0.4). It was found that the twinning fraction-strain curve followed a sigmoidal trend; consequently, saturation was expected to occur at strains exceeding 0.4. Based on the experimental data and the observed sigmoidal trend, an Avrami-type function was proposed to describe the dependence of twinning fraction on the app
- 26 September 2026
- Published by Elsevier in SSRN Electronic Journal
Open AccessCharacterization of a Novel Multicomponent High Entropy Steel with TWIP behavior: Design and Deformation behavior
In this research, a novel twinning-induced plasticity (TWIP) high entropy steel (HES) was designed using an approach combining thermodynamic criteria and multivariate optimization. The chemical composition was tailored to simultaneously satisfy the high entropy criterion, promote the formation of a single-phase fcc solid solution, and maintain the stacking fault energy within the appropriate range for the activation of the TWIP effect during deformation. Uniaxial compression tests were performed at strain levels of 0.1, 0.2, 0.3, and 0.4 and the corresponding microstructural evolutions were studied using optical microscopy and SEM-EBSD methods. The compressive yield stress of the material was determined to be 350 MPa. This value is at the upper limit of the yield stress of conventional TWIP steels. Three stages were identified in the work hardening rate ()-applied strain () curve. Stage I, appearing in the strain range ys<0.028 and characterized by a decrease in , was governed by rapid dislocation multiplication and slip. Stage II, appearing in the strain range 0.028<0.034, was characterized by an increase in value, due to the formation of initial twins, thereby obstructing dislocations. Stage III was characterized by a gradual decrease in , in the strain range of 0.1-0.4. In stage III, successive twinning waves occurred in the form of small "work-hardening bumps". The EBSD results confirmed that in the annealed (undeformed) sample, 39 % of the boundaries were annealing twin boundaries, and the rest were high-angle grain boundaries. With increasing applied strain, the fraction of twin boundaries first decreased to 16 % (at =0.1), due to the elongation of austenite grains and the partial transformation of annealing twins into high-angle boundaries, and then increased to 42 % (at =0.4). It was found that the twinning fraction-strain curve followed a sigmoidal trend; consequently, saturation was expected to occur at strains exceeding 0.4. Based on the experimental data and the observed sigmoidal trend, an Avrami-type function was proposed to describe the dependence of twinning fraction on the app
- Open Access
- 16 September 2026
- Published by Elsevier in SSRN Electronic Journal
Effect of binder architecture on densification, microstructural development, and quasi-static and dynamic compressive response of 92 wt.% tungsten heavy alloys containing Al and/or Ti
Binder architecture governs liquid-phase sintering and mechanical response in tungsten heavy alloys. Three 92 wt.% tungsten heavy alloys with Ni-Co-Fe-Al-Ti, Ni-Fe-Al, and Ni-free Co-Fe-Ti binders, designated W-NCFAT, W-NFA, and W-CFT, were produced by elemental powder milling, cold isostatic pressing, liquid-phase sintering at 1425 and 1455 °C under a controlled vacuum-H2-Ar atmosphere sequence, and vacuum dehydrogenation. Densification, tungsten grain morphology, binder continuity, elemental partitioning, contiguity, hardness, and compressive behavior were compared under identical processing conditions. The Ni-containing alloys reached 95.8–97.0% relative density and developed rounded tungsten grains separated by continuous metallic binder regions. W-CFT increased from 78.1% relative density at 1425 °C to 90.4% at 1455 °C, but retained substantial porosity, incomplete grain spheroidization, and discontinuous binder regions. W-NCFAT showed the highest hardness and reached a peak true compressive stress of 1255.4 MPa under quasi-static loading. W-NFA showed a lower peak stress but sustained a final true strain of 0.589 and a higher deformation energy density. In a representative split Hopkinson pressure bar test at approximately 2 × 10³ s⁻¹, W-NFA reached a converted true stress of 1020.7 MPa and remained intact to a final true strain of 0.344, whereas W-NCFAT reached 832.9 MPa at 0.065 before rapid load loss and fragmentation. EDS and XRD indicated continuous Ni-containing metallic binders, discrete Al/Ti-enriched oxygen-bearing constituents, dominant BCC tungsten, and weak reflections consistent with an FCC binder. For the investigated compositions and processing conditions, effective Al/Ti-containing binder performance was associated with sufficient Ni-assisted liquid-phase activity.
- 16 September 2026
- Published by Elsevier in SSRN Electronic Journal
Open AccessEffect of binder architecture on densification, microstructural development, and quasi-static and dynamic compressive response of 92 wt.% tungsten heavy alloys containing Al and/or Ti
Binder architecture governs liquid-phase sintering and mechanical response in tungsten heavy alloys. Three 92 wt.% tungsten heavy alloys with Ni-Co-Fe-Al-Ti, Ni-Fe-Al, and Ni-free Co-Fe-Ti binders, designated W-NCFAT, W-NFA, and W-CFT, were produced by elemental powder milling, cold isostatic pressing, liquid-phase sintering at 1425 and 1455 °C under a controlled vacuum-H2-Ar atmosphere sequence, and vacuum dehydrogenation. Densification, tungsten grain morphology, binder continuity, elemental partitioning, contiguity, hardness, and compressive behavior were compared under identical processing conditions. The Ni-containing alloys reached 95.8–97.0% relative density and developed rounded tungsten grains separated by continuous metallic binder regions. W-CFT increased from 78.1% relative density at 1425 °C to 90.4% at 1455 °C, but retained substantial porosity, incomplete grain spheroidization, and discontinuous binder regions. W-NCFAT showed the highest hardness and reached a peak true compressive stress of 1255.4 MPa under quasi-static loading. W-NFA showed a lower peak stress but sustained a final true strain of 0.589 and a higher deformation energy density. In a representative split Hopkinson pressure bar test at approximately 2 × 10³ s⁻¹, W-NFA reached a converted true stress of 1020.7 MPa and remained intact to a final true strain of 0.344, whereas W-NCFAT reached 832.9 MPa at 0.065 before rapid load loss and fragmentation. EDS and XRD indicated continuous Ni-containing metallic binders, discrete Al/Ti-enriched oxygen-bearing constituents, dominant BCC tungsten, and weak reflections consistent with an FCC binder. For the investigated compositions and processing conditions, effective Al/Ti-containing binder performance was associated with sufficient Ni-assisted liquid-phase activity.
- Open Access
- 24 July 2026
- Published by Elsevier in SSRN Electronic Journal
Effect of binder composition on densification, microstructural development, and quasi-static and dynamic compressive response of 92 wt.% tungsten heavy alloys containing Al and/or Ti
Binder composition governs liquid-phase sintering and mechanical response in tungsten heavy alloys. Three 92 wt.% tungsten heavy alloys with Ni-Co-Fe-Al-Ti, Ni-Fe-Al, and Ni-free Co-Fe-Ti binders, designated W-NCFAT, W-NFA, and W-CFT, were produced by elemental powder milling, cold isostatic pressing, liquid-phase sintering at 1425 and 1455 °C under a controlled vacuum-H2-Ar atmosphere sequence, and vacuum dehydrogenation. Densification, tungsten grain morphology, binder continuity, elemental partitioning, contiguity, hardness, and compressive behavior were compared under identical processing conditions. The Ni-containing alloys reached 95.8-97.0% relative density and developed rounded tungsten grains separated by continuous metallic binder regions. W-CFT increased from 78.1% relative density at 1425 °C to 90.4% at 1455 °C, but retained substantial porosity, incomplete grain spheroidization, and discontinuous binder regions. W-NCFAT showed the highest hardness and reached a peak true compressive stress of 1255.4 MPa under quasi-static loading. W-NFA showed a lower peak stress but sustained a final true strain of 0.589 and a higher deformation energy density. In a representative split Hopkinson pressure bar comparison at approximately 2 × 10³ s⁻¹, W-NFA reached a corrected true stress of 1020.7 MPa and remained intact to a final true strain of 0.344, whereas W-NCFAT reached 832.9 MPa at 0.065 before rapid load loss and fragmentation. EDS and XRD indicated continuous Ni-containing metallic binders, discrete Al/Ti-enriched oxygen-bearing constituents, dominant BCC tungsten, and weak reflections consistent with an FCC binder. Effective Al/Ti-containing binder modification therefore required sufficient Ni-assisted liquid-phase activity.
- 24 July 2026
- Published by Elsevier in SSRN Electronic Journal
Open AccessEffect of binder composition on densification, microstructural development, and quasi-static and dynamic compressive response of 92 wt.% tungsten heavy alloys containing Al and/or Ti
Binder composition governs liquid-phase sintering and mechanical response in tungsten heavy alloys. Three 92 wt.% tungsten heavy alloys with Ni-Co-Fe-Al-Ti, Ni-Fe-Al, and Ni-free Co-Fe-Ti binders, designated W-NCFAT, W-NFA, and W-CFT, were produced by elemental powder milling, cold isostatic pressing, liquid-phase sintering at 1425 and 1455 °C under a controlled vacuum-H2-Ar atmosphere sequence, and vacuum dehydrogenation. Densification, tungsten grain morphology, binder continuity, elemental partitioning, contiguity, hardness, and compressive behavior were compared under identical processing conditions. The Ni-containing alloys reached 95.8-97.0% relative density and developed rounded tungsten grains separated by continuous metallic binder regions. W-CFT increased from 78.1% relative density at 1425 °C to 90.4% at 1455 °C, but retained substantial porosity, incomplete grain spheroidization, and discontinuous binder regions. W-NCFAT showed the highest hardness and reached a peak true compressive stress of 1255.4 MPa under quasi-static loading. W-NFA showed a lower peak stress but sustained a final true strain of 0.589 and a higher deformation energy density. In a representative split Hopkinson pressure bar comparison at approximately 2 × 10³ s⁻¹, W-NFA reached a corrected true stress of 1020.7 MPa and remained intact to a final true strain of 0.344, whereas W-NCFAT reached 832.9 MPa at 0.065 before rapid load loss and fragmentation. EDS and XRD indicated continuous Ni-containing metallic binders, discrete Al/Ti-enriched oxygen-bearing constituents, dominant BCC tungsten, and weak reflections consistent with an FCC binder. Effective Al/Ti-containing binder modification therefore required sufficient Ni-assisted liquid-phase activity.
- Open Access
- 27 June 2026
- Published by Elsevier in SSRN Electronic Journal
Investigation into the effect of stress state on the ductile fracture of an aluminum-graphene oxide nanocomposite: numerical and experimental analyses
In this study, the effect of graphene oxide (GO) nanosheets on the fracture behavior of Al6061-GO nanocomposites was investigated. Tensile tests were carried out on smooth (without notch) and notched specimens with various weight percentages of GO (0.0%, 0.2%, 0.5% and 0.8%) to identify the fracture behavior of nanocomposites with different initial triaxiality levels. Microstructural observations showed that GO causes remarkable grain refinement in the Al6061 matrix. It was found that the grain refinement due to GO decreases the harmful effect of stress triaxiality on the fracture of composites. Furthermore, GO nanosheets can effectively deviate cracks, delaying their propagation and thus postponing the final fracture to larger strains. By using finite element simulation, a relationship was also established between the fracture strain, stress triaxiality level and wt. % of GO.
- 27 June 2026
- Published by Elsevier in SSRN Electronic Journal
Open AccessInvestigation into the effect of stress state on the ductile fracture of an aluminum-graphene oxide nanocomposite: numerical and experimental analyses
In this study, the effect of graphene oxide (GO) nanosheets on the fracture behavior of Al6061-GO nanocomposites was investigated. Tensile tests were carried out on smooth (without notch) and notched specimens with various weight percentages of GO (0.0%, 0.2%, 0.5% and 0.8%) to identify the fracture behavior of nanocomposites with different initial triaxiality levels. Microstructural observations showed that GO causes remarkable grain refinement in the Al6061 matrix. It was found that the grain refinement due to GO decreases the harmful effect of stress triaxiality on the fracture of composites. Furthermore, GO nanosheets can effectively deviate cracks, delaying their propagation and thus postponing the final fracture to larger strains. By using finite element simulation, a relationship was also established between the fracture strain, stress triaxiality level and wt. % of GO.
- 8 June 2026
- Published by SAGE Publications in Materials Science and Technology
Influence of heat treatment on microstructure and mechanical behavior of biocompatible MoNbTaTiZr high-entropy alloy
This study investigates the effect of aging temperature (1000–1300°C for 5 h) on a homogenized MoNbTaTiZr refractory high-entropy alloy. The homogenized microstructure comprised two BCC phases: dendritic BCC1 (hardness 4.66 GPa) and interdendritic BCC2 (hardness 2.56 GPa). Aging at 1100°C increased the BCC1 fraction to 86.8%, but further heating to 1300°C reduced it to 80.5% due to the formation of Ti/Zr-rich HCP precipitates. This precipitation raised the macro-hardness from 513 HV at 1000°C to 592 HV at 1300°C, despite a decrease in BCC1 micro-hardness from 493 to 417 HV. The results demonstrate that aging temperature critically controls phase evolution and mechanical properties.
- 8 June 2026
- Published by SAGE Publications in Materials Science and Technology
Influence of heat treatment on microstructure and mechanical behavior of biocompatible MoNbTaTiZr high-entropy alloy
This study investigates the effect of aging temperature (1000–1300°C for 5 h) on a homogenized MoNbTaTiZr refractory high-entropy alloy. The homogenized microstructure comprised two BCC phases: dendritic BCC1 (hardness 4.66 GPa) and interdendritic BCC2 (hardness 2.56 GPa). Aging at 1100°C increased the BCC1 fraction to 86.8%, but further heating to 1300°C reduced it to 80.5% due to the formation of Ti/Zr-rich HCP precipitates. This precipitation raised the macro-hardness from 513 HV at 1000°C to 592 HV at 1300°C, despite a decrease in BCC1 micro-hardness from 493 to 417 HV. The results demonstrate that aging temperature critically controls phase evolution and mechanical properties.
- Open Access
- 21 April 2026
- Published by Elsevier in SSRN Electronic Journal
Microstructure and mechanical behavior of as-cast AlMo0.5NbTa0.5TiZr refractory high-entropy alloy after aging at elevated temperatures
In this study, the effect of aging heat treatment on the microstructure, phase transformation, and mechanical properties of as-cast AlMo0.5NbTa0.5TiZr refractory high-entropy alloy has been investigated. The samples were directly aged (aging of the as-cast samples without prior homogenization) at 900, 1000, and 1100 °C for 2, 5, and 10 h. The results showed that increasing the aging time or temperature leads to a gradual homogenization of dendritic (DR) and interdendritic (IDR) regions, removing the elemental segregated regions as the coring effect and the formation and growth of secondary precipitates (mainly the Zr/Al-rich HCP phase). The X-ray diffraction analyses and thermodynamic simulations confirmed that the light elements (Al, Zr) tend to diffuse toward the IDR regions, while the heavy elements (Mo, Nb, Ta) remained inside the DR regions with BCC structure. The hardness measurements indicated that the maximum hardness (754 HV) is achieved after aging at 1000 °C for 5 h. The formation of fine HCP precipitates inside the DR phase and an increase in the fraction of IDR phase were found to be responsible for the increase in hardness. Further increase in the aging temperature or time caused the excessive coarsening of secondary precipitates and a dramatic decrease in the fracture toughness. This study indicated that the as-cast AlMo0.5NbTa0.5TiZr is thermally unstable and tends to decompose to a multi-phase structure.
- 21 April 2026
- Published by Elsevier in SSRN Electronic Journal
Open AccessMicrostructure and mechanical behavior of as-cast AlMo0.5NbTa0.5TiZr refractory high-entropy alloy after aging at elevated temperatures
In this study, the effect of aging heat treatment on the microstructure, phase transformation, and mechanical properties of as-cast AlMo0.5NbTa0.5TiZr refractory high-entropy alloy has been investigated. The samples were directly aged (aging of the as-cast samples without prior homogenization) at 900, 1000, and 1100 °C for 2, 5, and 10 h. The results showed that increasing the aging time or temperature leads to a gradual homogenization of dendritic (DR) and interdendritic (IDR) regions, removing the elemental segregated regions as the coring effect and the formation and growth of secondary precipitates (mainly the Zr/Al-rich HCP phase). The X-ray diffraction analyses and thermodynamic simulations confirmed that the light elements (Al, Zr) tend to diffuse toward the IDR regions, while the heavy elements (Mo, Nb, Ta) remained inside the DR regions with BCC structure. The hardness measurements indicated that the maximum hardness (754 HV) is achieved after aging at 1000 °C for 5 h. The formation of fine HCP precipitates inside the DR phase and an increase in the fraction of IDR phase were found to be responsible for the increase in hardness. Further increase in the aging temperature or time caused the excessive coarsening of secondary precipitates and a dramatic decrease in the fracture toughness. This study indicated that the as-cast AlMo0.5NbTa0.5TiZr is thermally unstable and tends to decompose to a multi-phase structure.
- 3 January 2026
- Published by Springer Nature in Metallurgical and Materials Transactions A
- Vol. 57 (3) , 981-999
Characterization of Microstructure and Flow Behavior of a Hot-Deformed Ni-Based Superalloy: Effect of Primary Heat Treatment
- 3 January 2026
- Published by Springer Nature in Metallurgical and Materials Transactions A
- Vol. 57 (3) , 981-999
Characterization of Microstructure and Flow Behavior of a Hot-Deformed Ni-Based Superalloy: Effect of Primary Heat Treatment
- 28 June 2024
- Published by Elsevier in Materials Science and Engineering: A
- Vol. 910
Hot deformation behavior and microstructural characterization of a novel high entropy steel
- 28 June 2024
- Published by Elsevier in Materials Science and Engineering: A
- Vol. 910
Hot deformation behavior and microstructural characterization of a novel high entropy steel