Abstract
Major improvements in the performance of aluminum-air batteries, based on improvement of the aluminum electrode polarization and limiting side reactions, are demonstrated. At high rates of discharge, cell performance is largely dictated by ohmic losses at the anode associated with the aluminum product layer. Turnover of this secondary passivation layer entails conversion of insoluble aluminum hydroxide to soluble aluminate ions. In cells employing the same air electrode and a polymer-based electrolyte, aluminum electrode behavior is systematically investigated as a function of hydroxide concentration, temperature, and electrolyte flow rate to identify optimum conditions and start-up protocols for battery discharge. Stannate addition and plating was explored as a path to inhibit Al corrosion and limit hydrogen evolution as a side reaction. The transient behavior of cells containing stannate in the electrolyte was studied to identify start-up conditions. Overall, this optimization enables a peak power density of 710 mW cm −2 in polarization experiments. Long-term constant current holds of the battery are also shown.
Funding Information
  • Army Research Laboratory (W911NF2220007)

This publication has 40 references indexed in Scilit: