Abstract
This study investigates the corrosion behaviour of hot-rolled A356 aluminium composites reinforced with Date Palm Seed Ash (DPSA), produced by gravity die casting, in 0.5 M NaOH solution using electrochemical techniques. The results showed that DPSA addition improved corrosion resistance compared to the unreinforced alloy, with optimal performance observed at 0.5–0.75 wt.% reinforcement. The 0.5 wt.% composite exhibited the highest polarisation resistance (2100 .cm2) and the largest capacitive response, while Tafel polarisation showed that 0.75 wt.% had the lowest corrosion current density (1.519 ×10-3 A/cm2), indicating optimum resistance in NaOH. SEM/EDX analysis confirmed improved surface integrity and reduced porosity for the optimised composite. The hot-rolled composites are suitable for structural applications in the process industry.