In-Vitro Comparison of Screw Loosening, Fracture Strength and Failure Mode of Implant-Supported Hybrid-Abutment Crowns and Screwmentable Crowns Manufactured with Different Materials
Authors:
Open Access
- 26 April 2025
- journal article
- research article
- Published by Wolters Kluwer Health in Nigerian Journal of Clinical Practice
- Vol. 28 (4) , 461-470
Abstract
Background: Hybrid-abutment crowns and screwmentable crowns offer a fusion of the benefits from both screw and cement-retained restorations, potentially enhancing the overall performance of the restoration. Aim: This study aimed to evaluate the screw loosening and fracture strength of hybrid-abutment crowns and screwmentable crowns made with two different materials. Methods: Forty single-crown were made on titanium implants and divided into four groups ( n = 10) [SM-Ti: Screwmentable titanium-porcelain crowns on stock titanium abutment; SM-Zr: Screwmentable zirconia-porcelain crowns on stock zirconia abutment; AC-Ti: Titanium-porcelain abutment crowns; AC-Zr: Zirconia-porcelain abutment crowns.] Specimens were torqued with 30 NCm and thermocycled between 5℃ and 55℃ in 20-second cycles for 5000 cycles. Removal torque values (RTV) were measured. Following the RTV measurement, the screws were changed with fresh screws and torqued again. Afterwards, specimens were loaded to fracture and fracture strengths were recorded, failure modes were examined. Statistical Analysis Used: Analysis of variance and Bonferroni test was performed. Results: The AC-Ti group displayed the highest mean torque loss (%20.09 ± 6.49) and the SM-Ti group displayed the lowest (%9.59 ± 8.84). Only the difference between AC-Ti and SM-Ti groups was found statistically significant, there are no significant differences between other groups. The fracture strengths are 385.84 ± 27.68 N, 313.18 ± 39.97 N, 272.69 ± 35.03 N, and 156.71 ± 19.83 N for AC-Ti, AC-Zr, SM-Ti, and SM-Zr groups, respectively and all differences were found to be statistically significant. Failures occurred as deformation in titanium components, whereas fractures were observed in zirconia components. Conclusion: Screw loosening was observed only in the AC-Ti group. No significant difference was observed among the torque loss values in the remaining groups. Titanium and zirconia materials do not exert any influence on screw loosening after thermal aging for hybrid-abutment crowns. Moreover, when assessing fracture strength, hybrid-abutment crowns exhibit superior strength and durability compared to screwmentable crowns.Keywords
This publication has 37 references indexed in Scilit:
- In Vitro Comparison of Modes of Failures among Titanium and One- and Two-piece Zirconia Abutment under Static LoadEuropean Journal of Dentistry, 2020
- Effect of fatigue loading on the fracture strength and failure mode of lithium disilicate and zirconia implant abutmentsClinical Oral Implants Research, 2017
- Effect of internal hexagonal index on removal torque and tensile removal force of different Morse taper connection abutmentsThe Journal of Prosthetic Dentistry, 2017
- Comparison of fracture strength and failure mode of different ceramic implant abutmentsThe Journal of Prosthetic Dentistry, 2017
- Fracture strength of implant abutments after fatigue testing: A systematic review and a meta-analysisJournal of the Mechanical Behavior of Biomedical Materials, 2016
- Comparison of fracture resistance of pressable metal ceramic custom implant abutment with a commercially fabricated CAD/CAM zirconia implant abutmentThe Journal of Prosthetic Dentistry, 2013
- Fracture resistance of titanium and zirconia abutments: An in vitro studyThe Journal of Prosthetic Dentistry, 2013
- Analysis of Changes in Implant Screws Subject to Occlusal Loading: A Preliminary AnalysisImplant Dentistry, 2005
- Virtual-Designed and Computer-Milled Implant AbutmentsJournal of Oral and Maxillofacial Surgery, 2005
- Thermal cycling procedures for laboratory testing of dental restorationsJournal of Dentistry, 1999