Corrosion Behavior of Solder Ribbon Caused by Acidification Inside Crystalline Si Photovoltaic Modules
Authors:
- 20 June 2021
- conference paper
- Published by Institute of Electrical and Electronics Engineers (IEEE)
- p. 2296-2298
Abstract
In crystalline-Si photovoltaic (PV) modules, a solder ribbon with a Cu core coated with solder is used as a connection with solar cells. Recent studies on the PV modules reported solder ribbon corrosion due to acetic acid generated by hydrolysis of EVA encapsulant. In this study, in order to understand the corrosion of the solder ribbon inside the PV modules, the corrosion of Sn plate and solder ribbon with respect to three kinds of carboxylic acids was investigated. The corrosion of Sn strongly depended on the pH of the aqueous solution. Furthermore, Sn luminescence was confirmed inside the PV modules.Keywords
This publication has 3 references indexed in Scilit:
- Influence of Front-Side Ag Metallization on High Temperature and High Humidity Test of Crystalline Silicon PV Module2019
- Optimization of thermo-mechanical reliability of solder joints in crystalline silicon solar cell assemblyMicroelectronics Reliability, 2016
- Field failure mechanism study of solder interconnection for crystalline silicon photovoltaic moduleMicroelectronics Reliability, 2012