Process-adapted temperature application within a two-stage rivet forming process for high nitrogen steel
Authors:
- 5 January 2022
- journal article
- research article
- Published by SAGE Publications in Proceedings of the Institution of Mechanical Engineers, Part L: Journal of Materials: Design and Applications
- Vol. 236 (6) , 1285-1301
Abstract
Mechanical joining technologies like self-piercing riveting are gaining importance with regard to environmental protection, as they enable multi-material design and lightweight construction. A new approach is the use of high nitrogen steel as rivet material, which allows to omit the usually necessary heat treatment and coating and thus leads to a shortening of the process chain. Due to the high strain hardening, however, high tool loads must be expected. Thus, appropriate forming strategies are needed. Within this contribution, the influence of applying different temperatures for each forming stage in a two-stage rivet forming process using the high nitrogen steel 1.3815 is investigated. The findings provide a basic understanding of the influence of the temperature management when forming high nitrogen steel. For this purpose, the rivets are not formed at the same temperature in each stage, but an elevated temperature is applied selectively. Different process routes are investigated. First, cups are manufactured in stage 1 at room temperature, followed by stage 2 at 200°C. Second, cups are formed in stage 1 at 200°C and used for stage 2 at room temperature. By comparing the findings with results when applying the same temperature in both stages, it is shown that the temperature during the first forming operation has an effect on the forming behaviour during the second forming stage. The required forming forces and the resulting rivet hardness can be influenced by process-adapted temperature application. Furthermore, the causes for the temperature impact on the residual cup thickness in stage 1 are evaluated by a cause and effect analysis, which provides a deeper process understanding. The thermal expansion of the tool and the billet as well as the improved forming behaviour at 200°C are identified as the main influencing causes on the achieved residual cup thickness.Keywords
Funding Information
- Deutsche Forschungsgemeinschaft (ME 2043/60-1; Project ID: 328853593)
This publication has 16 references indexed in Scilit:
- A review on mechanical joining of aluminium and high strength steel sheets by plastic deformationInternational Journal of Lightweight Materials and Manufacture, 2018
- Self-piercing riveting-a reviewThe International Journal of Advanced Manufacturing Technology, 2017
- Joining of dissimilar materialsCIRP Annals, 2015
- Self-piercing riveting (SPR) in the automotive industry: an overview2014
- Corrosion resistance of High nitrogen steels2012
- Handbuch Umformtechnik2010
- Self-piercing riveting of high tensile strength steel and aluminium alloy sheets using conventional rivet and dieJournal of Materials Processing Technology, 2009
- Plastic Joining of Ultra High Strength Steel and Aluminium Alloy Sheets by Self Piercing RivetCIRP Annals, 2006
- Springer Handbook of Materials Measurement Methods2006
- High Nitrogen Steels1999