Influence of distal-end heat treatment in the properties of heat-activated NiTi archwires
Authors:
- Janaína de Oliveira AbrahãoJAJanaína de Oliveira Abrahão
- Rodrigo Hermont CançadoRCRodrigo Hermont Cançado
- Esdras de Campos FrançaEFEsdras de Campos França
- Leandro de Arruda SantosLSLeandro de Arruda Santos
- Pedro Damas ResendePRPedro Damas Resende
- Felipe Weidenbach DegraziaFDFelipe Weidenbach Degrazia
- Leniana Santos NevesLNLeniana Santos Neves
- 27 August 2024
- journal article
- research article
- Published by Springer Nature in Journal of Orofacial Orthopedics / Fortschritte der Kieferorthopädie
- Vol. 86 (S1) , 31-38
Abstract
Purpose The aim of this study was to evaluate the extent of property changes caused by heating the distal portion of heat-activated nickel–titanium (NiTi) wires. Methods Forty preformed heat-activated NiTi archwires (3M Unitek, Monrovia, CA, USA) with a nominal cross-section of 0.018″ were used in this study. The archwires were divided into a control group, not submitted to heat treatment and, thus, maintaining the as-received properties, and an experimental group, in which the archwires were submitted to heat treatment for distal bending at one end. Wire segments of control and experimental groups were submitted to differential scanning calorimetry (DSC) and Vickers microhardness measurements. Results The DSC results suggest local recrystallization and precipitate dissolution at the heat-treated tip, which decreases as the distance to the wire’s tip increases. Vickers microhardness tests revealed significant changes for distances between 6 and 8 mm from the wire’s tip. Heating the distal portion of heat-activated NiTi archwires should be performed with care since this clinical procedure may compromise the performance of these wires to a distance of 8 mm from the archwire end. Conclusion Heat treatment for distal bending in heat-activated NiTi archwires may be performed, with little impact on the areas adjacent to heat treatment. In cases presenting molars requiring significant orthodontic corrections, it should be preferred to apply other techniques to avoid archwire sliding, such as crimpable stops, or to have flame control to avoid placing a heat-treated section in the tubes of these molars.Keywords
This publication has 25 references indexed in Scilit:
- Why do nickel-titanium archwires fracture intraorally? Fractographic analysis and failure mechanism of in-vivo fractured wiresAmerican Journal of Orthodontics and Dentofacial Orthopedics, 2007
- Temperature-modulated DSC provides new insight about nickel-titanium wire transformationsAmerican Journal of Orthodontics and Dentofacial Orthopedics, 2003
- Transformation Behavior, Chemical Composition, Surface Topography and Bending Properties of Five Selected 0.016'' × 0.022'' NiTi ArchwiresJournal of Orofacial Orthopedics / Fortschritte der Kieferorthopädie, 2003
- Pseudoelasticity and thermoelasticity of nickel-titanium alloys: A clinically oriented review. Part I: Temperature transitional rangesAmerican Journal of Orthodontics and Dentofacial Orthopedics, 2001
- An investigation into the effects of polishing on surface hardness and corrosion of orthodontic archwires.1999
- The Damon low-friction bracket: a biologically compatible straight-wire system.1998
- Differential scanning calorimetry (DSC) analyses of superelastic and nonsuperelastic nickel-titanium orthodontic wiresAmerican Journal of Orthodontics and Dentofacial Orthopedics, 1996
- Properties of superelastic wires and their relevance to orthodontic treatmentEuropean Journal of Orthodontics, 1995
- Bending properties of superelastic and nonsuperelastic nickel-titanium orthodontic wiresAmerican Journal of Orthodontics and Dentofacial Orthopedics, 1991
- An Evaluation of 55 Cobalt Substituted Nitinol Wire for Use in OrthodonticsThe Journal of the American Dental Association, 1971