Why do nickel-titanium archwires fracture intraorally? Fractographic analysis and failure mechanism of in-vivo fractured wires
Authors:
- Spiros ZinelisSpiros Zinelis
- Theodore EliadesTheodore Eliades
- Nikolaos PandisNPNikolaos Pandis
- George EliadesGEGeorge Eliades
- Christoph BourauelCBChristoph Bourauel
- 1 July 2007
- journal article
- research article
- Published by Elsevier in American Journal of Orthodontics and Dentofacial Orthopedics
- Vol. 132 (1) , 84-89
Abstract
No abstract availableKeywords
This publication has 18 references indexed in Scilit:
- Effect of fluoride prophylactic agents on the mechanical properties of nickel-titanium-based orthodontic wiresAmerican Journal of Orthodontics and Dentofacial Orthopedics, 2005
- Effect of acidic fluoride solution on β titanium alloy wireJournal of Biomedical Materials Research Part B: Applied Biomaterials, 2005
- Degradation of tensile strength of Ni–Ti superelastic alloy due to hydrogen absorption in methanol solution containing hydrochloric acidMaterials Science and Engineering: A, 2003
- Hydrogen embrittlement of Ni‐Ti superelastic alloy in fluoride solutionJournal of Biomedical Materials Research Part A, 2003
- Degradation and fracture of Ni–Ti superelastic wire in an oral cavityBiomaterials, 2001
- Surface characterization of retrieved NiTi orthodontic archwiresEuropean Journal of Orthodontics, 2000
- Hydrogen-enhanced localized plasticity—a mechanism for hydrogen-related fractureMaterials Science and Engineering: A, 1994
- Examination of Chinese NiTi wire by a combined clinical and laboratory approachEuropean Journal of Orthodontics, 1991
- Effect of long-term immersion corrosion on the flexural properties of nitinolAmerican Journal of Orthodontics, 1982
- Variable-modulus orthodonticsAmerican Journal of Orthodontics, 1981