Abstract
TaN thin films were grown by plasma-enhanced atomic layer deposition using tantalum-pentafluoride (TaF5)(TaF5) as the metal precursor and N2∕H2∕ArN2∕H2∕Ar plasma as the reducing agent at a temperature of 350°C350°C . When the source pulse time exceeded 1.5s1.5s , the thickness per cycle of TaN thin films was saturated at 0.41Å∕cycle0.41Å∕cycle and the resistivity was about 610μΩcm610μΩcm . Under this condition, the TaN thin films had a high density (14.6g∕cm3)(14.6g∕cm3) , which was very close to the theoretical value (15.8g∕cm3)(15.8g∕cm3) , and fluorine or hydrogen impurities were below detection limit. The resistivity and N∕TaN∕Ta ratio of the TaN thin films increased with the plasma time, and did not saturate. In addition, increasing the N2∕H2N2∕H2 ratio induced a sudden rise in the resistivity, which was related to the formation of a Ta3N5Ta3N5 phase. This dielectric phase was reduced by lowering the N2∕H2N2∕H2 ratio. In addition, when H2H2 plasma post-treatment was applied to the deposition process, the resistivity of the TaN thin films was reduced to 400μΩcm400μΩcm .
Keywords