Abstract
The wear resistance of TA15 titanium alloy can be significantly improved by the fabrication of TA15/WC-20Co composite tubes, showing promising application potential in aviation, transportation, and defense industries. However, the formation of brittle intermetallic compounds between TA15 and WC-20Co, coupled with their significant thermal expansion coefficient differences, poses challenges to enhancing interface bonding performance. In this work, the interface microstructure and interfacial bonding performance of TA15/WC-20Co composite tube with interlayer of V and Fe foils were studied. In addition, experimental characterization based on digital image correlation (DIC) and numerical simulation were carried out to investigate the residual stress in the TA15/WC-20Co composite tube. Results indicate that local shear strength decreases from top to bottom, with a maximum value of 294.5 MPa, while annular shear strength remains relatively uniform along the tube length, peaking at 230.5 MPa. Shear failure occurs at the V/Fe interface due to the presence of brittle V2C and V6C5 phases. The absolute value of the residual stress in the TA15 layer decreases radially outward. During the diffusion bonding stage (DBS), TA15 is subjected to granular medium loading, resulting in compressive principal stress dominated by S33 (σθ). In the cooling stage (CS), thermal contraction maintains compressive principal stress, mainly S11 (σR). Along the tube height during DBS, all stress components exhibit minimum absolute values in the mid-section. At CS, only S22 (σZ) shows the lowest magnitude in the middle region. The post-cooling compressive stress contributes to enhanced interfacial bonding strength. This study provides a theoretical basis for the fabrication and residual stress testing for TA15/WC-20Co composite tube.Keywords
This publication has 33 references indexed in Scilit:
- Influence of brazing temperature on microstructural characteristics and interfacial bonding strength in TA15/Ag-Cu-Ti (filler metal) /WC-xCo compositesCeramics International, 2025
- Effect of Diffusion Bonding Temperature on the Microstructure and Interfacial Shear Strength of TA15/Cemented Carbide Composite Plate with V/Fe Composite Intermediate LayersAdvanced Engineering Materials, 2025
- Establishment of a constitutive model for tungsten carbide with different cobalt content and grain size based on the split Hopkinson pressure bar impact testJournal of Mechanical Science and Technology, 2024
- Enhancing microstructure refinement and strengthening efficiency of TiBw/near α-Ti composites by combining solid-solution treatment with hot processingComposites Part B: Engineering, 2023
- Hole-Drilling Method for Deep Residual Stress Measure in Tensile Armour WiresExperimental Mechanics, 2022
- Effects of Pilger Rolling and Heat Treatment on Microstructure and Corrosion Resistance of Ag-Electroplated 304 Stainless Steel TubesMetals and Materials International, 2021
- Microstructural characteristics and mechanical properties of WC-Co/steel joints diffusion bonded utilizing Ni interlayerCeramics International, 2021
- Effect of microstructure on mechanical properties of net-structured TiBw/TA15 composite subjected to hot plastic deformationComposites Part B: Engineering, 2020
- Investigation of transverse residual stresses in a thick pultruded composite using digital image correlation with hole drillingComposite Structures, 2019
- Effect of internal pressure on springback during low pressure tube hydroformingInternational Journal of Material Forming, 2018