300 mm Wafer-scale In-situ CVD Growth Achieving 5.1×10-10 Ω-cm2 P-Type Contact Resistivity: Record 2.5×1021 cm-3 Active Doping and Demonstration on Highly-Scaled 3D Structures
Authors:
- 12 June 2022
- conference paper
- Published by Institute of Electrical and Electronics Engineers (IEEE)
- p. 367-368
Abstract
For the first time, we have developed a novel growth technique of Si1-xGex having active boron (B) doping concentration (NA) higher than 2×1021 cm-3. We achieve (1) uniform B doping and Ge composition in the epi-growth direction, (2) excellent uniformities in Si1-xGex thickness and resistivity across the entire 300 mm wafer, (3) an ultra-low as-deposited specific contact resistivity (ρc) of 5.1×10-10 Ω-cm2 on the sample with the highest NA of 2.5×1021 cm-3, and (4) successful selective growth on the advanced 3D structures with excellent conformality and thickness controllability.Keywords
This publication has 4 references indexed in Scilit:
- A Ladder Transmission Line Model for the Extraction of Ultralow Specific Contact Resistivity—Part II: Experimental VerificationIEEE Transactions on Electron Devices, 2020
- A Ladder Transmission Line Model for the Extraction of Ultralow Specific Contact Resistivity—Part I: Theoretical Design and Simulation StudyIEEE Transactions on Electron Devices, 2020
- (Invited)Laser Annealing in CMOS ManufacturingECS Transactions, 2018
- Thermal Stability of TiN/Ti/p+-Si0.3Ge0.7 Contact With Ultralow Contact ResistivityIEEE Electron Device Letters, 2017