Abstract
Several hurdles to further enhance the performance of semipolar III-Nitride laser diodes are addressed in this work. Particularly, we focused on improving their high operating voltage by thinning the p-GaN cladding layer and utilizing a transparent conductive oxide p-contact. On-wafer optical absorption measurements showed that a further reduction in voltage with thinner p-GaN was limited by increased optical loss due to increased mode overlap with the ITO/metal anode. In separate attempts to minimize bulk-related optical losses, we implemented a new design that consisted of an AlGaN electron blocking layer (EBL) placed remotely from the quantum wells (QWs) and a low p-waveguide Mg doping profile. A very low optical loss of about 2 cm-1 was extracted but the net improvement in differential efficiency was limited by lower internal injection efficiency due to carrier accumulation in the p-waveguide region. With an optimized design, that consisted of a lightly doped EBL close to the QWs and a UID p-waveguide, an improved light output power of 1.4 W at 1.5 A and a low threshold current density of 1.2 kA/cm2 were obtained.

This publication has 7 references indexed in Scilit: