Lubricant-Induced White Etching Cracks: Mechanism and Effects of Surface Finishing
- 1 August 2020
- book chapter
- Published by ASTM International
- p. 131-146
Abstract
Cylindrical roller thrust bearings (CRTBs) were fatigue tested in various lubricants under rolling-sliding conditions. The bearings exhibited premature damage when the tests were performed in a lubricant containing significant additives (referred to in this paper as “test gear oil”). Bearing life in the test gear oil was less than 5% of bearing life when tested in a mineral oil containing no additives. Investigations on posttest bearings from the test gear oil revealed localized raised areas on the tribosurfaces of the raceways. Upon further examination, subsurface white etching cracks (WECs) were observed beneath the raised surface features. The raised areas resembled hydrogen-induced blisters. Subsequent thermal desorption spectroscopy analysis of the bearing races with the raised features revealed hydrogen evolution from the posttest raceways. In contrast, races exhibited typical point surface origin (PSO)-type damage when the bearings were tested in plain mineral oil. Also, there were no subsurface crack networks or white etching features associated with the PSO spalling damage. Additional tests were performed with embedded abrasive particles that were introduced onto the raceways using a lapping process. Posttest investigations showed neither the raceways nor the rollers contained WECs, and the damage mode had changed even though they were tested in the test gear oil. Although WECs are generated in the subsurface, their formation depends on the surface condition of the raceways, so these results suggest that WEC formation is a surface-driven phenomenon. Based on these insights, possible WEC mitigation and prevention methods are discussed.Keywords
This publication has 23 references indexed in Scilit:
- Influence of Currents from Electrostatic Charges on WEC Formation in Rolling BearingsTribology Transactions, 2016
- White Etching Crack Root Cause InvestigationsTribology Transactions, 2014
- Three-dimensional imaging of hydrogen blister in iron with neutron tomographyActa Materialia, 2014
- A FIB/TEM study of butterfly crack formation and white etching area (WEA) microstructural changes under rolling contact fatigue in 100Cr6 bearing steelMaterials Science and Engineering: A, 2013
- Tribological advancements for reliable wind turbine performancePhilosophical Transactions of the Royal Society A: Mathematical, Physical and Engineering Sciences, 2010
- Tribology2009
- Hydrogen effects on the interaction between dislocationsActa Materialia, 1998
- Occurrence of brittle flaking on bearings used for automotive electrical instruments and auxiliary devicesWear, 1996
- Hydrogen-enhanced localized plasticity—a mechanism for hydrogen-related fractureMaterials Science and Engineering: A, 1994
- Hydrogen embrittlement of AISI 4130 steel with an alternate ferrite/pearlite banded structureMaterials Science and Engineering: A, 1991