Nonisothermal sintering of Cr2AlC powder

Authors:

Abstract
This work studies the sintering behavior of ultrafine powder of Cr2AlC compound during nonisothermal heating using a dilatometer. Sample exhibits relatively slower densification under pressureless condition where relative density increased from about 61% (green compact) to about 73% during heating up to 1350°C. Axial shrinkage data were analyzed through the volume diffusion and grain boundary diffusion‐based sintering models. Estimated activation energy of sintering (352kJ/mol) for volume diffusion mechanism, was found to be closely matching with the reported activation energy of chromium diffusivity, indicating volume diffusion as a controlling mechanism and chromium as a major diffuser in Cr2AlC.
Funding Information
  • SERB-DST (SR/S3/ME/0046/2012)

This publication has 27 references indexed in Scilit: