Experimental design to enhance the surface appearance, the internal structure, and the shear stresses of injected and metallized polycarbonate/acrylonitrile–butadiene‐styrene parts
- 22 August 2019
- journal article
- research article
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 137 (7)
Abstract
Polycarbonate (PC) and acrylonitrile–butadiene–styrene (ABS) possess thermal and mechanical properties, which make them materials of choice for automotive components. These properties have presented PC/ABS as an eligible replacement for metals in automotive industry. The aim of this study was to explore a new approach to determine the optimum conditions for obtaining quality and shear stresses of the injected and metalized PC/ABS parts. For this purpose, the following six injection‐molding parameters such as material temperature (137ma), injection pressure (Pinj), holding pressure (Ph), mold temperature (Tmo), holding time (th), and cooling time (tc) were considered at four different values. The effect of the injection parameters studied has been analyzed through the quality and the shear stresses values of the injected and metallized PC/ABS specimens. Optical microscopic and confocal laser scanning microscope (CLSM) results demonstrate that the occurrence of some defects such as weld line, blister, poor adhesion, metal residue, sand scratch. Moreover, scanning electron microscope (SEM) findings show the presence of core defects and solidified pellets. Shear stresses vary between 3.78 and 5.8 MPa for the injected specimens and 4.5 and 6.4 MPa for the metallized specimens. The optimum injection parameter combinations were conditioned by producing flawless injected and metallized PC/ABS parts having a significant shear stress value. Thus, the optimum combinations consists of: a Tma of 260 °C, a Pinj ranging between 30 and 50 bar, a Ph ranging between 20 and 25 bar, a Tmo of 40 °C, a th ranging between 8 and 14 sec. and a tc of 25 sec. These findings may have interesting applications in automotive part industry. © 2019 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2020, 137, 48384.Keywords
This publication has 33 references indexed in Scilit:
- Characterization of Thermo-Mechanical and Fracture Behaviors of Thermoplastic PolymersMaterials, 2014
- The use of Taguchi method in the design of plastic injection mould for reducing warpageJournal of Materials Processing Technology, 2007
- Application of Taguchi optimization technique in determining plastic injection molding process parameters for a thin-shell partMaterials & Design (1980-2015), 2007
- Comparison of the warpage optimization in the plastic injection molding using ANOVA, neural network model and genetic algorithmJournal of Materials Processing Technology, 2006
- Injection molding‐induced morphology of thermoplastic polymer blendsPolymer Engineering & Science, 2005
- Weld‐line characteristics of polycarbonate/acrylonitrile–butadiene–styrene blends. I. Effect of the processing temperatureJournal of Applied Polymer Science, 2004
- Optimal process conditions of shrinkage and warpage of thin‐wall partsPolymer Engineering & Science, 2004
- Effects of viscosity ratio and compatibilizers on the morphology and mechanical properties of polycarbonate/acrylonitrile‐butadiene‐styrene blendsPolymer Engineering & Science, 1999
- Fractography of injection molded polycarbonate acrylonitrile‐butadiene‐styrene terpolymer blendsPolymer Engineering & Science, 1992
- DISPERSION PHENOMENA IN HIGH VISCOSITY IMMISCIBLE FLUID SYSTEMS AND APPLICATION OF STATIC MIXERS AS DISPERSION DEVICES IN SUCH SYSTEMSChemical Engineering Communications, 1982