Yttria-Doped Zirconia-Hydroxyapatite Composite Coating on Cp-Ti Implants by Biomimetic Method
Authors:
- 24 January 2012
- journal article
- Published by Trans Tech Publications, Ltd. in Advanced Materials Research
- Vol. 445, 691-696
Abstract
Titanium (Ti) and Ti-alloys are often used in dental and orthopedic applications because of their good mechanical properties and biocompatibility. The advantages of Ti and Ti-alloys are its superior corrosion resistance, high fatigue strength and low elastic modulus which reduce stress shielding. Morover biocompatibility of them can be improved coating with bioceramics such as hydroxyapatite (HA) or other ceramic composites. The hydroxyapatite [Ca10(PO4)6(OH)2, H is frequently used as a coating material on the surfaces of Ti-based medical implants to improve the bone fixation and thus the lifetime of the implant is increased. However, the main weakness of HA lies on its poor mechanical strength that makes it unsuitable for load-bearing applications. An attractive way to produce the tougher HA is to use composite powders such as Yttria-Doped Zirconia-Hydroxyapatite (YSZ-HA) consisting of 8 mol% yttria-stabilized tetragonal zirconia (YSZ) so that the apatite phase increases the biocompatibility and zirconia (ZrO2) phase improves the strength. Y2O3 addition into zirconia can stabilize the tetragonal phase at room temperature (YSZ) and the tetragonal phase plays a major role to increase the fracture toughness. In the present study yttria-dopped zirconia powders by using ZrO(NO3)2.xH2O and Y(NO3)3.6H2O were produced to synthesize HA-YSZ composites. In accordance with this purpose, at the first step, Ca (NO3)2.4H2O, (NH4)2HPO4 and YSZ powders were dissolved in simulated body fluids (SBF) to obtain sol. The gelatin solutions with different concentration were added into sol to provide the gelation. Then the surfaces of Ti implants were soaked in this solution. The coating rate of Ti samples was arranged as 14 cm/s and coated implants were sintered at 900°C. Structural analysis of coated powders was obtained by using XRD. Morphological examinations and coating thickness were investigated by SEM. After the sol-gel solution was dried at 80°C, dried-powder was sintered at 900°C. Sintered powders were analyzed by FT-IR to determine any gelatin residue.Keywords
This publication has 13 references indexed in Scilit:
- Tailoring the Microstructure of Sol–Gel Derived Hydroxyapatite/Zirconia Nanocrystalline CompositesDiscover Nano, 2010
- Electrochemical and structural characterisation of zirconia reinforced hydroxyapatite bioceramic sol–gel coatings on surgical grade 316L SS for biomedical applicationsCeramics International, 2007
- Fluor-hydroxyapatite sol–gel coating on titanium substrate for hard tissue implantsBiomaterials, 2004
- The effect of sol–gel-formed calcium phosphate coatings on bone ingrowth and osteoconductivity of porous-surfaced Ti alloy implantsBiomaterials, 2004
- A simple biomimetic method for calcium phosphate coatingSurface and Coatings Technology, 2002
- Microstructural and mechanical study of zirconia-hydroxyapatite (ZH) composite ceramics for biomedical applicationsComposites Science and Technology, 2001
- Synthesis of biomimetic Ca-hydroxyapatite powders at 37°C in synthetic body fluidsBiomaterials, 2000
- New ideas in biomaterials science—a path to engineered biomaterialsJournal of Biomedical Materials Research, 1993
- Studies on the thermal spraying of apatite bioceramicsJournal of Thermal Spray Technology, 1992
- Osseointegrated Titanium Implants:Requirements for Ensuring a Long-Lasting, Direct Bone-to-Implant Anchorage in ManActa Orthopaedica, 1981