Burst tests of cold drawn and heat treated austenitic stainless steel (316L) tubes charged in pressurized hydrogen
Authors:
Preprint
- 19 February 2026
- preprint
- Published by Springer Nature in Research Square
Abstract
Global decarbonization targets are driving expansion of green hydrogen infrastructure, yet high-pressure hydrogen exposure can degrade the mechanical performance of critical stainless-steel components, typically made of the common steel 316L. This study evaluates the strength and fracture behaviour of both cold-drawn and heat treated 316L austenitic stainless-steel tubular specimens fabricated from 1/2" (12.7 mm) and 3/8" (9.53 mm) tube after gaseous high pressure pre-charging. Hydrogen concentration in the range between 76–100 ppm was measured in precharged sample in both states and the record of 2–5 ppm in the none-precharged specimen. Hydrostatic burst tests at ambient temperature were carried out with precharged specimens and revealed an increase in burst pressure for both material states, as compared to non-precharged specimens as a reference. In addition, fractographic analysis by scanning electron microscopy identified deeper dimples and wider microvoids in hydrogen-precharged specimens, indicating also some softening of the material in the cold drawn as well as in the heat-treated state. As the time to failure also increased, it is anticipated that the hydrogen introduced in the specimens caused a respective increase in both, ductility in terms of the straining and deformation capacity, as well as an increase in strength. For engineering applications, the findings indicate some beneficial effect that, despite exposure to extreme hydrogen conditions, 316L tubes retain, and even modestly enhance, their structural integrity, supporting a safe deployment in green hydrogen transport and storage systems, at least at ambient temperature.Keywords
All Related Versions
This publication has 21 references indexed in Scilit:
- Effect of Welding Microstructure on Stress Relaxation Cracking Studied by Controlled Residual Stress Generation in a 316L(N) Austenitic Stainless SteelMetallurgical and Materials Transactions A, 2023
- The synergistic action and interplay of hydrogen embrittlement mechanisms in steels and iron: Localized plasticity and decohesionEngineering Fracture Mechanics, 2019
- Effect of Boron Content on Hot Ductility and Hot Cracking Susceptibility in 316L Austenitic Stainless Steel for Welding ComponentsJournal of Materials Engineering and Performance, 2018
- Hydrogen influence on some advanced high-strength steelsCorrosion Science, 2017
- Hydrogen Embrittlement UnderstoodMetallurgical and Materials Transactions A, 2015
- Hot cracking tests—an overview of present technologies and applicationsWelding in the World, 2014
- Hydrogen-Assisted Crack Propagation in Austenitic Stainless Steel Fusion WeldsMetallurgical and Materials Transactions A, 2009
- Creep deformation and fracture behavior of types 316 and 316L(N) stainless steels and their weld metalsMetallurgical and Materials Transactions A, 2000
- The effect of hydrogen on the yield and flow stress of an austenitic stainless steelMetallurgical and Materials Transactions A, 1995
- Hydrogen-induced strain localization and failure of austenitic stainless steels at high hydrogen concentrationsActa Metallurgica et Materialia, 1991