Failure Prediction of Lithium Disilicate and Composition-Gradient Multilayered Zirconia Occlusal Veneers: A Fractographic and Theoretical Analysis
Open Access
- 12 September 2025
- Vol. 18 (18) , 4287
Abstract
This in vitro study aimed to evaluate the fatigue behavior of occlusal veneers (OVs) made of lithium disilicate and composition-gradient multilayered zirconia at different thicknesses, incorporating both experimental and theoretical analyses to predict long-term performance. Seventy-two OVs with ceramic layer thicknesses of 0.5 mm, 1.0 mm, and 1.5 mm were fabricated and adhesively bonded to dentin analog composite abutments. All specimens underwent thermomechanical fatigue testing, involving cyclic loading (49 N, 1.6 Hz, 1.2 million cycles) and thermocycling (5–55 °C), simulating five years of clinical function. Fracture patterns were analyzed using light microscopy and scanning electron microscopy. A fatigue lifetime model based on plate-on-foundation theory and slow crack growth was applied to estimate cycles to radial failure. No complete fractures or debonding occurred. However, 50% of 0.5 mm zirconia OVs developed flexural radial cracks from the intaglio surface, while all lithium disilicate and zirconia veneers ≥1.0 mm remained intact. Theoretical predictions closely matched the experimental outcomes, indicating that 0.5 mm zirconia performance aligned with the lower-bound fatigue estimates for 5Y-PSZ. Results suggest that lithium disilicate offers superior fatigue resistance at minimal thickness, while thin zirconia is prone to subsurface cracking. A minimum thickness of 0.7 mm is recommended for zirconia-based OVs.Keywords
Funding Information
- Ivoclar Vivadent (n/a)
- National Institutes of Health (1R01DE033545-28, 1R01DE026279-24)
This publication has 45 references indexed in Scilit:
- Recent advances in dental zirconia: 15 years of material and processing evolutionDental Materials, 2024
- An investigation on fatigue, fracture resistance, and color properties of aesthetic CAD/CAM monolithic ceramicsClinical Oral Investigations, 2022
- Effect of preparation design on marginal adaptation and fracture strength of ceramic occlusal veneers: A systematic reviewClinical and Experimental Dental Research, 2022
- Impact of different layers within a blank on mechanical properties of multi-layered zirconia ceramics before and after thermal agingDental Materials, 2022
- ADM guidance—Ceramics: guidance to the use of fractography in failure analysis of brittle materialsDental Materials, 2017
- Effect of the microstructure on the lifetime of dental ceramicsDental Materials, 2011
- Slow crack growth and reliability of dental ceramicsDental Materials, 2011
- Approach for valuating the influence of laboratory simulationDental Materials, 2009
- Residual stresses in bilayer dental ceramicsBiomaterials, 2005
- Elastic contact versus indentation modeling of multi-layered materialsInternational Journal of Solids and Structures, 1992