Effect of oxidation on wear resistance of 3D-printed titanium alloy Ti-6Al-4V parts
Authors:
- Oksana EvtushenkoOEOksana Evtushenko
- Marina KazachenokMKMarina Kazachenok
- Dmitriy BuslovichDmitriy Buslovich
- Sergey MartynovSMSergey Martynov
- 19 November 2019
- conference paper
- Published by AIP Publishing in AIP Conference Proceedings
- Vol. 2167 (1) , 020094
Abstract
Low wear resistance is one of the disadvantages of both wrought and additive manufactured titanium alloys. At present paper the effect of thermal oxidation at a temperature of 700 °С during 4h and 8h on the wear resistance and friction coefficient in 3D printed samples of Ti-6Al-4V alloy is studied. Ti–6Al–4V parts were produced by electron beam free-form fabrication process. Bilayer oxide (TiO2/Al2O3,) formed on the surface of 3D printed of Ti–6Al–4V samples during oxidation was revealed using X-ray diffraction method. It was shown that the thermal oxidation significantly decreases the wear rate of the Ti–6Al–4V samples. A two-stage dependence of friction coefficient on the sliding distance was demonstrated. The wear mechanisms of 3D printed of Ti–6Al–4V samples and bilayer oxide were discussed.This publication has 5 references indexed in Scilit:
- Multiscale Deformation of Commercial Titanium and Ti一6Al-4V Alloy Subjected to Electron Beam Surface TreatmentPhysical Mesomechanics, 2018
- Plasma electrolytic oxidation of titanium in a phosphate/silicate electrolyte and tribological performance of the coatingsApplied Surface Science, 2014
- Tribological behavior of Ti-6Al-4V and Ti-6Al-7Nb Alloys for Total Hip ProsthesisAdvances in Tribology, 2014
- Oxidation of Ti–6Al–4V alloyJournal of Alloys and Compounds, 2009
- Dry sliding wear mechanisms of the Ti6Al4V alloyWear, 1997