SMSergei A. Martynov

Sergei A. Martynov

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article

Previous Organizations / Institutes

The organizations / institutes from the scholar's other articles in the past ten years


Sergei A. Martynov has a total of 67 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Structural Phase State, Martensitic Transformations and Inelastic Properties of TiNi-based Alloy Fabricated by Electron Beam Wire-Feed Additive Manufacturing

    by K. V. Krukovskii, D. Yu. Zhapova, S. A. Martynov, Yu. P. Mironov, A. V. Kim, A. A. Gusarenko

    In this paper, the structural phase state, martensitic transformation temperatures, and inelastic properties of a TiNi-based alloy obtained by electron beam wire-feed additive manufacturing (EBAM) on a Ti49.8Ni50.2 (at %) substrate were studied. It was shown that the printed samples had an inhomogeneous coarse-grained microstructure both in the direction perpendicular and parallel to the substrate. The microstructure type of the samples obtained by EBAM depends on the distance from the substrate and is determined by the cooling conditions in the vacuum chamber of the setup for 20 h from 800°C. At room temperature, the obtained samples had a high-temperature B2-phase structure. It was established that the printed samples underwent a B2 ↔ B19' martensitic transformation upon cooling and heating. It was shown that the studied samples exhibit a superelasticity of 9.01% under torsion with an accumulated plastic strain of 1.28% (including 5.78% in the absence of plastic deformation).

  • Effect of Titanium and Titanium Nickelide Substrates on the Structural-Phase State and Mechanical Properties of Electron Beam Additive Manufacturing TiNi-Based Alloys

    by D. Yu. Zhapova, K. V. Krukovskii, Yu. P. Mironov, S. A. Martynov, A. V. Kim, I. A. Danilov

    We investigated the structural-phase state and mechanical properties of a TiNi-based alloy, obtained by electron beam wire-feed additive manufacturing on titanium and titanium nickelide substrates. It was shown that the printed samples have a heterogeneous coarse-grained microstructure. At room temperature, the obtained samples have the structure of the high-temperature B2-phase of TiNi and the secondary Ti2Ni (or Ti4Ni2Ox) phase. It was found that the printed samples on the Grade 2 substrate failed brittlely during testing. The printed samples on Ti49.8Ni50.2 (at %) substrate were plastically deformed and demonstrated pseudoelasticity plateau. It is shown that the value of mechanical properties correlates with the content of Ti2Ni (or Ti4Ni2Ox).

  • Open Access

    Transformations of the Microstructure and Phase Compositions of Titanium Alloys during Ultrasonic Impact Treatment Part III: Combination with Electrospark Alloying Applied to Additively Manufactured Ti-6Al-4V Titanium Alloy

    by Alexey Panin, Marina Kazachenok, Konstantin Krukovskii, Dmitry Buslovich, Lyudmila Kazantseva, Sergey Martynov, Elena Sklyarova

    Scanning electron microscopy, 3D optical surface profilometry, as well as X-ray diffraction and electron backscatter diffraction analysis were implemented for studying the effects of both ultrasonic impact treatment (UIT) and ultrasonic impact electrospark treatment (UIET) procedures on the microstructure, phase composition, as well as the mechanical and tribological properties of Ti-6Al-4V samples fabricated by wire-feed electron beam additive manufacturing. It was shown that he UIET procedure with the WC-6%Co striker enabled to deposit the ~10 µm thick coating, which consists of fine grains of both tungsten and titanium-tungsten carbides, as well as titanium oxide. For the UIET process, the effect of shielding gas on the studied parameters was demonstrated. It was found that the UIET procedure in argon resulted in the formation of a dense, continuous and thick (~20 µm) coating. After the UIET procedures in air and argon, the microhardness levels were 26 and 16 GPa, respectively. After tribological tests, wear track surfaces were examined on the as-built sample, as well as the ones subjected to the UIT and UIET procedures. It was shown that the coating formed during UIET in air had twice the wear resistance compared to the coating formed in argon. The evidence showed that the multiple impact of a WC-Co striker with simultaneous electrical discharges was an effective way to improve wear resistance of the Ti-6Al-4V sample.


  • Open Access

    Deformation Behavior of Wrought and EBAM Ti-6Al-4V under Scratch Testing

    by Artur Shugurov, Alexey Panin, Marina Kazachenok, Lyudmila Kazantseva, Sergey Martynov, Alexander Bakulin, Svetlana Kulkova

    The microstructure, mechanical properties, and deformation behavior of wrought and electron beam additive manufactured (EBAM) Ti-6Al-4V samples under scratching were studied. As-received wrought Ti-6Al-4V was subjected to thermal treatment to obtain the samples with microstructure and mechanical characteristics similar to those of the EBAM samples. As a result, both alloys consisted of colonies of α phase laths within prior β phase grains and were characterized by close values of hardness. At the same time, the Young’s modulus of the EBAM samples determined by nanoindentation was lower compared with the wrought samples. It was found that despite the same hardness, the scratch depth of the EBAM samples under loading was substantially smaller than that of the wrought alloy. A mechanism was proposed, which associated the smaller scratch depth of EBAM Ti-6Al-4V with α′→α″ phase transformations that occurred in the contact area during scratching. Ab initio calculations of the atomic structure of V-doped Ti crystallites containing α or α″ phases of titanium were carried out to support the proposed mechanism.


  • Open Access

    Effects of Water Cooling on the Microstructure of Electron Beam Additive-Manufactured Ti-6Al-4V

    by Alexey Panin, Sergey Martynov, Marina Kazachenok, Lyudmila Kazantseva, Alexander Bakulin, Svetlana Kulkova, Olga Perevalova, Elena Sklyarova

    The inferior mechanical properties of EBAM Ti-6Al-4V samples are due to the coarse columnar grains containing coarse lamellar structures. One can expect that water cooling of the build platform will increase the cooling rate of the molten pool during the build-up process, causing microstructure refinement. In the present work, the substrate cooling effects on the microstructure and phase composition of EBAM Ti-6Al-4V samples are studied using optical, scanning electron, and scanning transmission microscopy, as well as X-ray diffraction analysis. It is shown that the microstructure of the EBAM Ti-6Al-4V samples built on the substrate without water cooling consists predominantly of columnar prior β grains with lateral sizes ranging up to 2000 µm, while cooling of the build platform causes the appearance of equiaxed prior β grains measuring 1000 µm. Moreover, the refinement of the martensite structure and the precipitation of α′′ martensite platelets within α laths occur in the EBAM Ti-6Al-4V samples built on the water-cooled build platform. An explanation of the mechanisms underlying the α′→α + β and α′→α + α′′ + β transformations during the building process is provided based upon ab initio calculations. The fragmentation of the α laths under the residual compressive stresses is discussed.


  • Electron beam additive manufacturing of TiCx/Ti-6Al-4V composite

    by Artem Builuk, Marina Kazachenok, Sergey Martynov

    In this paper, the technology of simultaneous electron beam melting of the titanium alloy wire of Ti-6Al-4V and TiC powder was developed. The effect of 3D printing parameters on the microstructure and mechanical properties of TiCх/Ti-6Al-4V composites was also investigated. Simultaneous feeding of the Ti-6Al-4V wire and the TiCx/Ti-6Al-4V mechano-composite leads to a change in the microstructure of the 3D-printed samples. Such a change in the microstructure leads to a significant increase in the microhardness and mechanical characteristics under tension. The maximum ultimate tensile strength (950 MPa) and ductility (6%) are achieved with the introduction of the mechano-composite TiC15wt%/Ti-6Al-4V.


  • Effect of oxidation on wear resistance of 3D-printed titanium alloy Ti-6Al-4V parts

    by Oksana Evtushenko, Marina Kazachenok, Dmitriy Buslovich, Sergey Martynov

    Low wear resistance is one of the disadvantages of both wrought and additive manufactured titanium alloys. At present paper the effect of thermal oxidation at a temperature of 700 °С during 4h and 8h on the wear resistance and friction coefficient in 3D printed samples of Ti-6Al-4V alloy is studied. Ti–6Al–4V parts were produced by electron beam free-form fabrication process. Bilayer oxide (TiO2/Al2O3,) formed on the surface of 3D printed of Ti–6Al–4V samples during oxidation was revealed using X-ray diffraction method. It was shown that the thermal oxidation significantly decreases the wear rate of the Ti–6Al–4V samples. A two-stage dependence of friction coefficient on the sliding distance was demonstrated. The wear mechanisms of 3D printed of Ti–6Al–4V samples and bilayer oxide were discussed.


  • Electron beam additive manufacturing of TiB2/Ti–6Al–4V composite

    by Alexey Panin, Marina Kazachenok, Lyudmila Kazantseva, Sergey Martynov, Michail Korchagin

    Microstructure and phase composition of the titanium matrix composite made from a pre-mixed powder blend of Ti–6Al–4V+TiB2 were studied. High energy planetary ball milling method was used both to obtain TiB2 powder and to mix Ti–6Al–4V matrix composite powder with 5 wt.% TiB2. Electron beam melting technology was used to build the parts of the titanium metal matrix composites. To modify the microstructure of additive manufactured TiB2/Ti–6Al–4V sample their surface layer was subjected to one-pass electron beam melting. It was shown that the microstructure of 3D- printed TiB2/Ti–6Al–4V sample consists of equiaxial prior β grains of approximately 200 µm in size with the acicular α phase. TiB phase formation in the as-build titanium matrix composite was found. Subsequent electron beam surface treatment decreased in the width of acicular α phase and increased in the volume fraction of β phase in the titanium matrix composite.


  • Effect of microstructure on mechanical properties and deformation behavior of Ti–6Al–4V alloy during scratch testing

    by Artur R. Shugurov, Marina S. Kazachenok, Sergey A. Martynov, Artur M. Kasterov, Elena A. Sinyakova

    The phase composition, mechanical properties and deformation behavior under scratch testing of Ti–6Al–4V alloy samples with different microstructure were studied. It was found that the volume fraction of the β-Ti in the sample with bimodal microstructure was nearly twice as low as that in the samples with lamellar and globular microstructure. The sample with bimodal microstructure was characterized by increased hardness and hardness to Young’s modulus ratio (H/E) as compared with other samples. The residual depth of the scratch grooves in the Ti–6Al–4V alloy samples was shown to be in a good agreement with the H/E ratio.