Trivalent chromium process (TCP) is one of the promising alternatives to chromate conversion coating (CCC). For the CCC process, the main electroactive component of the solution is Cr6+ [1]. In the TCP solution, the main components are Cr3+ and ZrF62- [2]. Due to environmental and health concerns, non-chromate coating systems are developed. For example, fluorozirconate coating systems contain Zr4+ (ZrF62-) and small amounts of non-chromium metal ions, such as TiF62- and Zn2+ [3]. In response to international regulations, TCP is also expected to be replaced. However, it is interesting why ZrF62- is the main component of commercial TCP solutions. In this study, 7075-T6 Al alloys were treated in Cr3+ conversion solutions without and with 0.0005 M F- for 1, 10, and 30 min. SEM characterization revealed that the morphology of 7075-T6 Al after conversion coating in Cr3+ solutions was similar to the counterpart after alkaline degreasing and acidic desmutting. Moreover, the Cr signal was not acquired in EDS spectrums. The polarization curves recorded in 0.5 M Na2SO4 + 0.05 M NaCl showed insignificant inhibition in anodic and cathodic kinetics. A protective conversion coating cannot grow in Cr3+ solutions with 0.0005 M F-. However, a protective conversion coating formed in the Cr3+ solution with a higher F- concentration. The 7075-T6 Al alloy treated in the Cr3+ solution containing 0.072 M F- for 1 min exhibited inhibited anodic and cathodic kinetics. Cross-sectional TEM characterization revealed the formation of a 30-nm-thick, Cr-rich coating. As a result, the continuous, thin Cr-rich coating confers corrosion resistance. However, a local corrosion attack was observed on the sample with extended conversion coating treatments. Grain boundaries of 7075-T6 were etched severely after 10 min of conversion coating treatment. Large corrosion spots appeared after 30 min of conversion coating treatment. Consequently, F- facilitates the conversion coating reaction in Cr3+ solutions via the attack of the substrate. However, F- can have negative effects on the continuity and integrity of the coating, specifically extended treatment in the solution with larger F- concentrations. Reference: Suib, S. L., La Scala, J., Nickerson, W., Fowler, A., & Zaki, N. (2009). Determination of hexavalent chromium in NAVAIR trivalent chromium process (TCP) coatings and process solutions. Metal Finishing, 107(2), 28-34. Munson, C. A., et al. (2018). "Cross comparison of TCP conversion coating performance on aluminum alloys during neutral salt-spray and thin-layer mist accelerated degradation testing." Electrochimica Acta282: 171-184 Milošev, I., & Frankel, G. S. (2018). Conversion coatings based on zirconium and/or titanium. Journal of The Electrochemical Society, 165(3), C127-C144.