Abstract
NiO films were grown on Si(100) by atomic layer deposition using Ni(Cp)2Ni(Cp)2 ( Cp=cyclopentadienylCp=cyclopentadienyl , C5H5C5H5 ) or Ni(EtCp)2Ni(EtCp)2 [ EtCp=ethylcyclopentadienylEtCp=ethylcyclopentadienyl , (C2H5)(C5H4)(C2H5)(C5H4) ] and ozone in the 150–300°C150–300°C temperature range. The growth temperature dependence of structure, electronic density, and impurity levels for the prepared NiO films was studied using X-ray reflectivity, X-ray diffraction (XRD), Fourier transform infrared (FTIR) spectroscopy, time of flight–secondary ion mass spectroscopy (ToF-SIMS), and transmission electron microscopy. The behavior of films deposited using Ni(Cp)2Ni(Cp)2 and Ni(EtCp)2Ni(EtCp)2 is compared and discussed. NiO films with good stoichiometry and low amounts of contaminants are obtained at a growth temperature (Tg)(Tg) of 250°C250°C or above. At a fixed TgTg , the growth rate for NiO films deposited using Ni(Cp)2Ni(Cp)2 is higher than the one of films deposited using Ni(EtCp)2Ni(EtCp)2 . Furthermore, the growth rate for NiO deposited using Ni(Cp)2Ni(Cp)2 at Tg=150°CTg=150°C is 0.32nm∕cycle0.32nm∕cycle and decreases substantially in films deposited at higher temperatures. The electronic density of NiO films deposited at 300°C300°C is close to the one of bulk NiO (1.83e−∕Å3)(1.83e−∕Å3) . According to XRD and FTIR results, films deposited at Tg⩾200°CTg⩾200°C have a simple cubic polycrystalline structure. Impurities in NiO films decrease with increasing TgTg , as detected by ToF-SIMS.

This publication has 42 references indexed in Scilit: