Influence of Overheating on High-Cycle Fatigue Characteristics of the Base Metal and Weld Metal of Low-Carbon Steel Welded Joints
Authors:
- Sergey A. NikulinSNSergey A. Nikulin
- Stanislav O. RogachevSRStanislav O. Rogachev
- Dmitriy V. ProsvirninDPDmitriy V. Prosvirnin
- Svetlana V. PivovarchikSPSvetlana V. Pivovarchik
- Vladislav A. BelovVBVladislav A. Belov
- Nikolay V. ShplisNSNikolay V. Shplis
- Mikhail Y. ZadorozhnyyMZMikhail Y. Zadorozhnyy
- Vladimir M. KhatkevichVKVladimir M. Khatkevich
Open Access
Abstract
The results of a high-cycle fatigue testing of our samples were obtained, and a comparative assessment of the properties of the base metal and weld metal of 09G2S-type steel (13Mn6 according to the DIN17145-80 standard) before and after overheating (1200 °C, 3.7 h) was performed. The welded joints between the sheets of 09G2S steel were obtained through automatic argon arc welding. The fatigue tests were carried out under repeated tensile loading. The “maximum cycle stress—number of cycles to failure” fatigue curves of the samples were plotted. The fracture surfaces of the samples were studied, and the fatigue failure mechanisms were analyzed. It was shown that, during testing, all samples demonstrated cyclic hardening behavior. The samples of the base metal as delivered had the highest endurance limit, and the smallest endurance limit was found in the samples of the base metal and weld metal after overheating, the endurance limits of which were similar. The fracture mechanism of all samples was quasi-brittle with the presence of very thin fatigue micro-grooves. The final rupture of all samples had a ductile dimple type.Keywords
This publication has 29 references indexed in Scilit:
- Strength of steel for unique engineering structuresRussian Metallurgy (Metally), 2012
- Cumulative fatigue damage in low cycle fatigue and gigacycle fatigue for low carbon–manganese steelInternational Journal of Fatigue, 2011
- Effect of Microstructure on Fatigue Crack Propagation and S–N Fatigue Behaviors of TMCP Steels with Yield Strengths of Approximately 450 MPaMetallurgical and Materials Transactions A, 2010
- High-cycle fatigue failure of low-carbon steel after long-term agingInorganic Materials, 2010
- Extremely low cycle fatigue tests on structural carbon steel and stainless steelJournal of Constructional Steel Research, 2010
- The severe accident mitigation concept and the design measures for core melt retention of the European Pressurized Reactor (EPR)Nuclear Engineering and Design, 2004
- Micromechanisms of fatigue crack nucleation and short crack growth in a low carbon steel under low cycle impact fatigue loadingInternational Journal of Fatigue, 1999
- High cycle fatigue of low alloy carbon steelsJournal of Materials Processing Technology, 1997
- Fatigue striation in a wide range of crack propagation rates up to 70 ?m/cycle in a ductile structural steelJournal of Materials Science, 1980
- Review: Fatigue-crack propagation in metallic and polymeric materialsJournal of Materials Science, 1972