Latest Publications

  • Effect of High-Temperature Exposure on Low-Carbon Steel Welded Joint Metal Fracture Toughness

    by S. A. Nikulin, S. O. Rogachev, V. A. Belov, N. V. Shplis, V. Yu. Turilina, L. V. Fedorenko, A. V. Molyarov, D. Yu. Ozherelkov

  • Open Access

    Influence of Overheating on High-Cycle Fatigue Characteristics of the Base Metal and Weld Metal of Low-Carbon Steel Welded Joints

    by Sergey A. Nikulin, Stanislav O. Rogachev, Dmitriy V. Prosvirnin, Svetlana V. Pivovarchik, Vladislav A. Belov, Nikolay V. Shplis, Mikhail Y. Zadorozhnyy, Vladimir M. Khatkevich

    The results of a high-cycle fatigue testing of our samples were obtained, and a comparative assessment of the properties of the base metal and weld metal of 09G2S-type steel (13Mn6 according to the DIN17145-80 standard) before and after overheating (1200 °C, 3.7 h) was performed. The welded joints between the sheets of 09G2S steel were obtained through automatic argon arc welding. The fatigue tests were carried out under repeated tensile loading. The “maximum cycle stress—number of cycles to failure” fatigue curves of the samples were plotted. The fracture surfaces of the samples were studied, and the fatigue failure mechanisms were analyzed. It was shown that, during testing, all samples demonstrated cyclic hardening behavior. The samples of the base metal as delivered had the highest endurance limit, and the smallest endurance limit was found in the samples of the base metal and weld metal after overheating, the endurance limits of which were similar. The fracture mechanism of all samples was quasi-brittle with the presence of very thin fatigue micro-grooves. The final rupture of all samples had a ductile dimple type.


  • Open Access

    Structure and properties of steels for manufacture of core catcher vessel of nuclear reactor

    by S. A. Nikulin, S. O. Rogachev, V. A. Belov, N. V. Shplis, A. A. Komissarov, V. Yu. Turilina, Yu. A. Nikolaev

    The Russian new nuclear reactors are provided with a special core catcher vessel device (cc-vessel) designed to minimize the consequences of a severe beyond design basis accident at a nuclear power plant, when the reactor pressure vessel collapses and the core melts. For manufacture of the cc-vessel structural elements, low-carbon unalloyed or low-alloyed steels are used. When a severe beyond design basis accident develops, the cc-vessel’s body is subjected to extreme temperature and force loads, which can lead to degradation of the structure, loss of strength and failure of the entire cc-vessel. To calculate the strength characteristics of the cc-vessel, which ensure its safe and reliable operation, the detailed data are required on the structure and mechanical properties of low-carbon steels at high temperatures and after extreme thermal actions simulating the development of a severe beyond design basis accident. The paper analyzes data on the structure and mechanical properties (tensile strength, crack resistance, toughness and cyclic strength) of a number of low-carbon steels under extreme temperature and force actions, including conditions simulating the development of a severe beyond design basis accident at a nuclear power plant, in order to select the material for the design of cc-vessel of nuclear reactor. New data on the structure, mechanical properties, and thermal diffusivity in a wide temperature range of a Cr – Mo steel (Russian Standard – 15KhM) as a candidate structural material for the manufacture of the cc-vessel body are presented. The low content of manganese and alloying with molybdenum and vanadium in 15KhM steel provides a finer grained structure and eliminates the steel’s tendency to temper brittleness.


  • Impact Strength of Low-Carbon Steel 09G2S Welded Joint Metal

    by S. A. Nikulin, S. O. Rogachev, V. A. Belov, A. A. Komissarov, V. Yu. Turilina, N. V. Shplis, Yu. A. Nikolaev


  • Open Access

    Effect of Prolonged Thermal Exposure on Low-Cycle Bending Fatigue Resistance of Low-Carbon Steel

    by Sergey A. Nikulin, Stanislav O. Rogachev, Vladislav A. Belov, Mikhail Y. Zadorozhnyy, Nikolay V. Shplis, Mikhail M. Skripalenko

    Using a dynamic mechanical analyzer, the comparative studies of a low-cycle bending fatigue were carried out for AISI 1022 low-carbon steel after extreme thermal exposure, simulating the severe beyond-design-basis accident at nuclear power plants. In the as-delivered state, the steel has a high resistance to low-cycle fatigue (the fatigue strength at N = 3.5 × 104 cycles (σNf) was 360 MPa). Long-term thermal exposure led to a slight decrease in the resistance to low-cycle fatigue of steel: σNf is decreased by 9%. The influence of AISI 1022 steel structure on the characteristics of fatigue strength and fracture mechanisms is analyzed.


  • Open Access

    Influence of long-term high-temperature action on impact toughness of base metal and weld metal of 22K steel welded joint

    by S. A. Nikulin, S. O. Rogachev, V. A. Belov, A. A. Komissarov, V. Yu. Turilina, N. V. Shplis, Yu. A. Nikolaev

    One of the applications of construction low-carbon 22K steel (AISI 1022 type) is as a material for the vessel of a core catcher (CC) for nuclear power plants with VVER reactors. In the event of severe beyond design basis accident, the CC-vessel will be under conditions of prolonged hightemperature impacts, which can significantly change the structural state and lead to degradation of mechanical properties of the vessel material. Data on the effect of such actions on the mechanical properties and fracture resistance of welds (the properties of which usually differ from those of the base metal) from low-carbon steels are very limited in the literature. This makes it difficult to guarantee the reliability and safety prediction of CC. The purpose of this work was to carry out the comparative Charpy V-notch impact tests of the samples of base metal and weld metal of the 22K steel welded joint before and after long-term high-temperature heat treatment, simulating the thermal effect on the reactor vessel material of nuclear power plants during severe accidents. Welded joints of 22K steel sheets were obtained by the method of automatic argon-arc welding with a consumable electrode (welding wire SV-08G2S was used) in accordance with PNAE G-7-009–89. Based on the test results, the ductile–brittle transition curves were plotted and analysis of fracture surfaces after tests was carried out. The influence of structural factors on the impact toughness has been studied. It is shown that prolonged high-temperature exposure leads to an increase in the temperatures of beginning and end of the ductile-brittle transition by 30 – 50 °C and to the expansion of range of the ductile-brittle transition temperature by 15 – 25 °C of both base metal and weld metal of the welded joint.


  • Influence of Long-Term High-Temperature Action on the Impact Toughness of the Base Metal and the Weld Metal of the 22K Steel Welded Joint

    by S. A. Nikulin, S. O. Rogachev, V. A. Belov, A. A. Komissarov, V. Yu. Turilina, N. V. Shplis, Yu. A. Nikolaev

    One of the applications of construction low-carbon 22K steels (AISI 1022 type) is used as a material for the body of a core catcher (CC) for nuclear power


  • Increasing of the information and technology efficiency of superjet diagnostics by sequential hydrodynamic exposure on the material

    by A. A. Barzov, V. A. Belov, K. A. Bogdanov

    The sequential hydroerosive local destruction of the surface layer of the material, first with a high and then low pressure superjet it is possible to obtain additional information about its ability to withstand external fatigue-damaging effects is shown in the paper. A new parameter that characterizes the structural stability of the properties of the diagnosed materials is proposed and experimental confirmation of its information and technological significance is carried out.