Multiphase Mixed Material Derived From Calcite and Diammonium Hydrogen Phosphate Coated With Tetraethyl Orthosilicate: A Potential Implant Coating Material
Authors:
- Emmanuel Obeng AgyenEAEmmanuel Obeng Agyen
- Kezia Yaa AwortweKAKezia Yaa Awortwe
- Bernard Owusu AsimengBABernard Owusu Asimeng
- Claude Fiifi HayfordCHClaude Fiifi Hayford
- Ralph KwakyeRKRalph Kwakye
- Kwabena Kan-DapaahKKKwabena Kan-Dapaah
- Lily PaemkaLPLily Paemka
Open Access
- 1 January 2025
- journal article
- Published by Wiley in Advances in Materials Science and Engineering
- Vol. 2025 (1)
Abstract
A multiphase mixed material (M‐PMM) made from calcite and diammonium hydrogen phosphate was prepared using the wet chemical method. To improve its bioactivity, the M‐PMM was coated with tetraethyl orthosilicate (TEOS) at varying mass percentages of 5% and 10% producing 5%_TEOS‐M‐PMM and 10%_TEOS‐M‐PMM, respectively. In vitro mineralization studies were conducted by immersing the uncoated M‐PMM, 5%_TEOS‐M‐PMM, and 10%_TEOS‐M‐PMM in simulated body fluid (SBF) for days 7, 14, and 21. Characterization of the uncoated and coated M‐PMM was performed using X‐ray diffractometry (XRD), Fourier transform infrared spectroscopy (FTIR), energy dispersion X‐ray spectroscopy (EDS), X‐ray fluorescence (XRF), and scanning electron microscopy (SEM). The uncoated M‐PMM was confirmed to consist of multiple phases, including calcite, mixed type‐AB carbonate hydroxyapatite, and hydroxyapatite monoclinic2 by XRD and FTIR. EDS also confirmed the presence of silicon at the surface of the coated M‐PMM, whereas XRD showed a decrease in crystallinity and crystallite size. The crystallinity and crystallite size were 81% and 20.88 ± 5.12 nm for uncoated M‐PMM, respectively. The coated M‐PMM had values of 79% and 17.27 ± 9.06 nm and 78% and 19.83 ± 9.91 nm for 5%_TEOS‐M‐PMM and 10%_TEOS‐M‐PMM, respectively. The larger surface area of the coated M‐PMM in the SBF gave a better resorption of calcium and phosphate minerals, which was confirmed by XRF. Apatite‐like bundles in the uncoated M‐PMM and coated M‐PMM after immersion in SBF from day 7 to day 21 were revealed by SEM. However, additional cuboid structures were seen in the coated M‐PMM, which enhanced its cell viability and will aid in better osteointegration with biological tissues.Keywords
This publication has 50 references indexed in Scilit:
- Characterization of Enhanced UHMWPE ‐Hap Composites Manufactured by Hot PressingPolymer Composites, 2025
- A Review on High Entropy Alloys as Metallic Biomaterials: Fabrication, Properties, Applications, Challenges, and Future ProspectsBiomedical Materials & Devices, 2025
- Hybrid coatings on dental and orthopedic titanium implants: Current advances and challengesBMEMat, 2024
- Characterisation of TEOS-Based Sol–Gel-Hydroxyapatite Composite Coating on Titanium ImplantsBiomedical Materials & Devices, 2024
- Whole blood stimulation as a tool for studying the human immune systemEuropean Journal of Immunology, 2023
- Methods of Chemical Synthesis in the Synthesis of Nanomaterial and Nanoparticles by the Chemical Deposition Method: A ReviewBioNanoScience, 2022
- Vascularization in tissue engineering: The architecture cues of pores in scaffoldsJournal of Biomedical Materials Research Part B: Applied Biomaterials, 2021
- Substituted hydroxyapatites for bone regeneration: A review of current trendsJournal of Biomedical Materials Research Part B: Applied Biomaterials, 2016
- Infrared spectroscopic characterization of carbonated apatite: A combined experimental and computational studyJournal of Biomedical Materials Research Part A, 2013
- Recent Progress on Silica Coating of Nanoparticles and Related NanomaterialsAdvanced Materials, 2010