Structure, mechanical properties, and corrosion resistance of low-nickel nitrogen-alloyed austenite stainless steel
Open Access
- 1 January 2026
- journal article
- Published by National Library of Serbia in Journal of Mining and Metallurgy, Section B: Metallurgy
- Vol. 62 (00) , 6
Abstract
This study investigates the structure, mechanical properties, and corrosion resistance of low-nickel nitrogen-alloyed austenitic stainless steels (Cr17Mn9Ni3N, 05Cr18Mn10Ni3N) as cost-effective alternatives to conventional AISI 304L and AISI 321 grades. The alloys were smelted in vacuum induction melting with nitrogen introduced via nitrided ferrochrome. Microstructural analysis confirmed fully austenitic structures with finer grain sizes (ASTM No. 4.5-6.0) compared to conventional steels (ASTM No. 3.5-4.0). Mechanical testing revealed superior yield strength (~414 MPa) and tensile strength (~730-748 MPa) in nitrogen-alloyed steels, attributed to solid-solution strengthening by nitrogen. However, the impact toughness at cryogenic temperatures (-196°C) was reduced, and brittle facets were found on the fracture surface. The results of potentiodynamic polarization tests showed that AISI 304L steel exhibited a higher pitting potential. The pitting potentials of steels Cr17Mn9Ni3N and 05Cr18Mn10Ni3N were lower than that of AISI 304L but higher than that of AISI 321 steel. Economic analysis highlighted significant cost savings potential through nickel substitution with nitrogen. The results validate nitrogen-alloyed steels as viable alternatives for applications requiring high strength and corrosion resistance, though cryogenic applications require careful nickel content optimization.Keywords
This publication has 24 references indexed in Scilit:
- Nickel-saving Type High Nitrogen Austenitic Stainless Steel2022
- Development of High-Strength Corrosion Resistant Austenitic Steel for Oil Equipment ShaftsMetallurgist, 2022
- Melting of High-Nitrogen Austenitic Steels at Atmospheric PressureMetallurgist, 2019
- Impact Toughness Properties of Nickel- and Manganese-Free High Nitrogen Austenitic Stainless SteelsMetallurgical and Materials Transactions A, 2016
- Effect of alloying elements on ductile-to-brittle transition behavior of high-interstitial-alloyed 18Cr-10Mn austenitic steelsProcedia Engineering, 2011
- Effects of deformation-induced martensite and grain size on ductile-to-brittle transition behavior of austenitic 18Cr-10Mn-N stainless steelsMetals and Materials International, 2010
- Microstructure of nitrogen implanted stainless steel after wear experimentSurface and Coatings Technology, 2007
- High Nitrogen Austenitic Stainless Steels Manufactured by Nitrogen Gas Alloying and Adding Nitrided FerroalloysJournal of Iron and Steel Research International, 2007
- Nitrogen Containing Austenitic Stainless SteelsMaterialwissenschaft und Werkstofftechnik, 2006
- High Nitrogen Steels1999