Mechanical, fracture toughness, and Dynamic Mechanical properties of twill weaved bamboo fiber‐reinforced Artocarpus heterophyllus seed husk biochar epoxy composite
- 4 September 2022
- journal article
- research article
- Published by Wiley in Polymer Composites
- Vol. 43 (11) , 8388-8395
Abstract
This research aimed to find the effect of Artocarpus heterophyllus fruit seed husk biochar (ASB) and twill weaved bamboo fiber (TBF) in mechanical, DMA, and fracture toughness behavior of epoxy‐based composite. The surface of both weaved bamboo fiber and biochar was treated with amino silane before composite making. In this investigation, the laminates were fabricated by hand layup process and analyzed by appropriate ASTM standards. Results of this study revealed that the incorporation of 40 vol.% twill weaved bamboo fiber (EB) into the resin improved the mechanical properties. The load distribution was uniform with twilled weaving. For composite designation EBJ3, the maximum measured tensile strength was 168 MPa, the tensile modulus is 6.24 GPa, the flexural strength is 195 MPa, and the flexural modulus is 6.85 GPa, the izod impact is 6.24 J, and the hardness is 90 shore‐D. Similarly, the maximum storage modulus and lowest loss factor for the composite designation EBJ3 were measured to be 3.8 GPa and 0.4, respectively. Moreover, the maximum measured fracture toughness and energy release rate is 39.4 MPa.√m and 0.88 MJ/m2 for composite designation EBJ3 with 5.0% biochar and 40% bamboo fibers in volume. The SEM fractography revealed that the matrix molecules are adhered to the fiber, indicating enhanced bonding. These biomass waste converted fruit seed husk biochar and industrial crop bamboo fiber epoxy composites could be used as workable material in structural, defense, automotive, and domestic product‐making applications.Keywords
This publication has 31 references indexed in Scilit:
- Thermal and Mechanical Properties of Bamboo Fiber Reinforced Epoxy CompositesPolymers, 2018
- Mechanical Strength Behaviour of Silane Treated E-glass Fibre/Al 6061 & SS-304 Wire Mesh Reinforced Epoxy Resin Hybrid CompositeSilicon, 2018
- Effect of Silane Modified E-glass Fibre/Iron(III)Oxide Reinforcements on UP Blended Epoxy Resin Hybrid CompositeSilicon, 2018
- Effect of alkali treatment on wettability and thermal stability of individual bamboo fibersJournal of Wood Science, 2018
- Biochar potential evaluation of palm oil wastes through slow pyrolysis: Thermochemical characterization and pyrolytic kinetic studiesBioresource Technology, 2017
- Plasticizing effect of coconut oil on morphological, mechanical, thermal, rheological, barrier, and optical properties of poly(lactic acid): A promising candidate for food packagingJournal of Applied Polymer Science, 2017
- Fibre prestressed composites: Theoretical and numerical modelling of unidirectional and plain-weave fibre reinforcement formsComposite Structures, 2017
- Thermo-mechanical characterization of siliconized E-glass fiber/hematite particles reinforced epoxy resin hybrid compositeApplied Surface Science, 2016
- Radio frequency shielding behaviour of silane treated Fe2O3/E-glass fibre reinforced epoxy hybrid compositeApplied Physics A, 2016
- Mechanical properties of partially pyrolysed composites with plain weave basalt fibre reinforcementCeramics International, 2014