Effect of Simulated Tooth Temperature on the Degree of Conversion of Self-adhesive Resin Cements Exposed to Different Curing Conditions
Authors:
Open Access
- 1 March 2014
- journal article
- research article
- Published by Operative Dentistry in Operative Dentistry
- Vol. 39 (2) , 204-212
Abstract
This study evaluated the degree of conversion (DC) of two commercial, self-adhesive resin cements (SARCs) using Fourier transform infrared analysis (FTIR) polymerized at simulated prepared tooth surface temperatures and under different curing conditions. RelyX U100 (U100, 3M ESPE) and Maxcem Elite (MX, Kerr Corporation) were mixed at 25°C and applied to the surface of a horizontal attenuated total reflectance (ATR) unit, which was near room temperature (RT, control) (25°C) or heated to simulate prepared tooth surface temperatures (28°C and 32°C) and then attached to an infrared spectrometer. The products were polymerized using one of three conditions: direct light exposure through a glass slide (DLE), exposure through a 1.5-mm thick ceramic disc overlay (CO) (A2 shade, IPS e.max, Ivoclar Vivadent), or self-curing (SC). FTIR spectra were recorded for 12 minutes (1 spectrum/s, 16 scans/spectrum, resolution 4 cm−1) immediately after application to the ATR. The DC was calculated using standard techniques of observing changes in aliphatic-to-aromatic peak ratios before and 12 minutes after curing, as well as during each 1-second interval. DC data (n=7) were analyzed by two-way analysis of variance and Tukey's post-hoc test (p=0.05). Both simulated tooth temperatures significantly increased DC in all groups of MX and in the CO and SC groups of U100 compared with the RT control. For MX, the self-cure groups exposed to tooth temperatures showed DC values similar to those of the CO groups. For U100, the CO groups showed higher DC values than SC groups regardless of temperature. Time-based conversion profiles ranged according to product, temperature, and curing mode. Causing SARCs to polymerize at simulated tooth temperatures increases DC of SARCs compared with room-temperature curing values, mainly in the SC mode.Keywords
This publication has 13 references indexed in Scilit:
- Influence of the Curing Mode on Fluoride Ion Release of Self-adhesive Resin Luting Cements in Water or During pH-Cycling RegimenOperative Dentistry, 2012
- Pre-heated dual-cured resin cements: analysis of the degree of conversion and ultimate tensile strengthBrazilian Oral Research, 2011
- Self-adhesive resin cements - chemistry, properties and clinical considerationsJournal of Oral Rehabilitation, 2010
- Curing efficiency of four self-etching, self-adhesive resin cementsDental Materials, 2009
- Effect of sodium sulfinate salts on the polymerization characteristics of dual-cured resin cement systems exposed to attenuated light-activationJournal of Dentistry, 2009
- Kinetic analysis of monomer conversion in auto- and dual-polymerizing modes of commercial resin luting cementsThe Journal of Prosthetic Dentistry, 2009
- Effect of Curing Method and Storage Condition on Fluoride Ion Release from a Fluoride-releasing Resin CementDental Materials Journal, 2006
- Calibration of FTIR conversion analysis of contemporary dental resin compositesDental Materials, 1990
- Correlation of Parameters used to Estimate Monomer Conversion in a Light-cured CompositeJournal of Dental Research, 1988
- The feasibility of temperature measurement as a diagnostic procedure in human teethJournal of Dentistry, 1986