Nitriding of FeAl40 (Fe–40 at.%Al) intermetallic high-temperature alloy allows improving its anti-wear properties. Such nitriding leads to the formation of an outer white layer composed of iron nitrides and an inner diffusion zone with precipitated AlN. In the present work, gaseous nitriding was performed at 590 °C over a wide range of nitriding potentials and treatment times. The specimens have been investigated by scanning electron microscopy supplemented by electron backscatter diffraction, electron probe microanalysis, transmission electron microscopy and X-ray diffraction. These measurements reveal the microstructure evolution and form the basis for explaining the observed layer growth kinetics on the basis of an internal nitriding mechanism governed by inwards diffusion of N and immediate precipitation of lamellar AlN. The compressive stress induced by the nitriding leads to previously reported out-diffusion of preferably Fe developing the white layer, but also to the formation of Fe-rich wave-like features developing by Fe diffusion to grain boundaries oriented parallel to the surface. It is argued that the high interface density obviously facilitates these diffusive processes, since Fe volume diffusion is not sufficiently rapid to account for the observed diffusion lengths. With increasing nitriding potentials also appreciable regions of the diffusion layer transform to iron nitrides. Notably, the ε-iron nitrides develop in the lamellar AlN-containing regions, whereas the Fe-rich wave-like features transform to γ′-iron nitrides. It is likely the presence of Al and/or microstructural constraints that prevent the formation of the γ′-iron nitrides in the case of the lamellar AlN-containing regions.

This publication has 52 references indexed in Scilit: