Abstract
Anion exchange membrane water electrolyzer (AEMWE) with non-noble metal catalyst and electrolyzer components and energy efficiency close to proton exchange membrane water electrolyzer (PEMWE) is suitable to reduce the cost of green hydrogen. [1] The lack of membrane durability is the fundamental issue for the commercialization of AEMWE. [2] The durability of AEMs are depend on the stability of polymeric back bone and the ion exchange group. Earlier, to improve the performance of AEMWE, AEM with high ion exchange capacity (IEC) was used. However, high IEC increases the membrane swelling, thereby leading to poor mechanical stability. It is important to address the trade-off between the performance and durability of the AEM. In this point, we found that increasing π–π stacking between the polymeric backbone chains effectively reduces the swelling of the AEMs with high IEC. In this work, we present the effect of π–π interaction between the polymeric backbone on the durability and hydrogen crossover of the AEM. We developed two types of AEMs, PFT-C 10 -TMA [3] (Figure 1a) and PFT-C 6 -TMA-C 1 (Figure 1b), both have aromatic backbone and aliphatic side chains with ion exchange group, and having similar IEC values (2.7 meq/g). PFT-C 6 -TMA-C 1 AEM has aromatic groups with shorter aliphatic side chains (C 6 ) with ion exchange group and (C1) without ion exchange groups in the polymeric backbone, leading to the formation of π–π interaction. Membrane electrode assemblies (MEA) were prepared using these membranes, and their durability and hydrogen gas crossover were tested. Under similar test conditions, the MEA with PFT-C 6 -TMA-C 1 showed lower hydrogen crossover than the MEA based on PFT-C 10 -TMA (Figure 1c). Furthermore, the PFT-C 6 -TMA-C 1 membrane showed stable performance in load cycle durability tests conducted between 0.1–3 A/cm 2 at 80 °C. These results suggest that PFT-C 6 -TMA-C 1 membrane has stronger π–π stacking between the polymeric backbone chains, which increases the durability and reduces the hydrogen gas crossover for AEMWE. Acknowledgement This presentation is based on results obtained from a project, JPNP20003, commissioned by the New Energy and Industrial Technology Development Organization (NEDO), Japan. References A. Miller, K. Bouzek, J. Hnat, S. Loos, C.I. Bernäcker, T. Weißgärber, L. Röntzsch, J. Meier-Haack, Sustain. Energy Fuels, 4 , 2114–2133 (2020). Li, A.R. Motz, C. Bae, C. Fujimoto, G. Yang, F. Y. Zhang, K. E. Ayers, Y. S. Kim, Energy Environ. Sci., 14 , 3393- 3419 (2021). Miyanishi, T. Yamaguchi, Polym. Chem., 11 , 3812–3820, (2020) Figure 1. Chemical structures of (a) PFT-C 10 -TMA, (b) PFT-C 6 -TMA-C 1 . (c) Hydrogen crossover values of PFT-C 10 -TMA and PFT-C 6 -TMA-C 1 membrane based MEAs measured by performing electrolysis at 2A/cm 2 and in 1 M KOH at 80°C. Figure 1